CVD Diamond | Superior CVD Lab Grown Diamonds for High-Performance Optical Applications
Optical CVD Diamond Specification
Next-Gen Photonic Material for Extreme Environments
Dominating optical performance with the industry’s widest transmission band (225 nm - 25 μm, skip 1.8-2.5 μm), CVD single-crystal diamond adds microwave transparency to its unique portfolio. Unmatched radiation resistance, Vickers hardness >100 GPa, 2,200 W/mK thermal conductivity, chemical stability, and ultra-low expansion establish it as the benchmark IR window material.
Critical Parameters
┌────────────────────────┐
│ Parameter │ Specification │
├────────────────────────┤
│ Refractive Index │ ~2.4 (1-30 μm optimal) │
│ Surface Roughness │ Ra <50 nm (post-polish) │
│ Dimensional Error │ ≤0.2 mm │
│ Key Geometry │ Mid-IR triangular prisms │
└────────────────────────┘
Application Matrix
-
Energy Systems: CO₂ lasers / Gyrotron RF generators
-
Imaging & Sensing: LWIR (8-14 μm) detectors / Raman spectrometers
-
Micro-Optics: Diamond lenses for miniaturized systems
-
Research Frontiers: Extreme-environment optical components
Transformative Advantages
-
Scatter Suppression: <0.1% light loss at 10 μm wavelength
-
Material Efficiency: 30% weight reduction vs. ZnSe optics
-
Failure Resistance: Zero corrosion in acidic/alkaline media
-
Design Freedom: Enables previously impossible optical configurations
|
Refractive Index (1064nm)
|
2.392
|
|
Refractive Index (600nm)
|
2.415
|
|
Transmission (1064nm)
|
>68%
|
|
Transmission (8μm-25μm)
|
>70%
|
|
Thermal Conductivity
|
>2000 W/mK
|
|
Crystallographic Orientation
|
100 110 111
|
|
Miscut for Main Face Orientation
|
±3°
|
|
Common Product Size
|
2mm×2mm×6mm
2mm×2mm×7mm 4mm×4mm×7mm |
|
Transverse Tolerance
|
±0.05mm
|
|
Thickness Tolerance
|
±0.1mm
|
|
Parallelism
|
<2′
|
|
Surface Roughness
|
<10nm
|
|
Edge Cutting
|
Laser Cutting
|
Get in Touch