OEM Custom 6mm Nylon Kevlar Cord Belts - 3.2kg Tensile Strength, 1.5-3% Stretch Rate for Industrial Applications
Price:
Negotiable
MOQ:
1200 Meter
Delivery Time:
Within 5 working days After receipt of your deposit
Brand:
Jiuna
Product Description
Product Overview
Custom OEM reinforced cord belts available in 6mm nylon and Kevlar constructions, designed for demanding industrial applications requiring superior strength and minimal stretch.
Kevlar Belt Features
- Available in round or V-section profiles
- Low stretch with excellent anti-abrasion properties
- Cogged options available for increased flexibility
- Easily made endless using Drive welding kits
Technical Specifications
| Diameter (mm) | Min. Radius (in/mm) | Stretch Rate | Max. Tensile (kg/lbs) | Hardness (A) | Roll Length (m) |
|---|---|---|---|---|---|
| 5mm | 1.57in / 40mm | 1.5-3% | 2.0kg / 4.3lbs | 85 | 100 |
| 6mm | 1.97in / 50mm | 1.5-3% | 3.2kg / 7.0lbs | 85 | 100 |
| 7mm | 2.17in / 55mm | 1.5-3% | 4.1kg / 9.0lbs | 85 | 100 |
| 8mm | 2.56in / 65mm | 1.5-3% | 5.0kg / 11.0lbs | 85 | 100 |
| 9mm | 2.95in / 75mm | 1.5-3% | 6.8kg / 15.0lbs | 85 | 50 |
| 10mm | 2.95in / 75mm | 1.5-3% | 7.7kg / 17.0lbs | 85 | 50 |
| 12mm | 3.94in / 100mm | 1.5-3% | 12.2kg / 27.0lbs | 85 | 30 |
| 15mm | 4.72in / 120mm | 1.5-3% | 17.7kg / 39.0lbs | 85 | 30 |
| 18mm | 5.71in / 145mm | 1.5-3% | 25.4kg / 56.0lbs | 85 | 30 |
| 20mm | 6.30in / 160mm | 1.5-3% | 31.3kg / 69.0lbs | 85 | 30 |
Industrial Applications
- Elevator slide shaft systems
- Medium to heavy-duty industrial applications
- Conveying and diverging operations including product sizing
- Material handling for wood, laminate, roof and ceiling tile
Quality for keeping going, Credit to win the world
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.