U Bending ASTM A213 TP304L Stainless Steel For Boiler and Heat Exchanger
U Bending ASTM A213 TP304L Stainless Steel For Boiler and Heat Exchanger
Chemical composition
|
America standard |
European standard |
C % max |
Mn % max |
P % max |
S % max |
Si % max |
Cr % |
Ni % |
Mo% |
|
TP304 |
1.4301 |
0.080 |
2.0 |
0.045 |
0.03 |
1.00 |
18.00-20.00 |
8.00-11.00 |
- |
|
TP304L |
1.4307 |
0.035 |
2.0 |
0.045 |
0.03 |
1.00 |
18.00-20.00 |
8.00-12.00 |
- |
|
TP304H |
/ |
0.04-0.10 |
2.0 |
0.045 |
0.03 |
1.00 |
18.00-20.00 |
8.00-11.00 |
- |
Mechanical properties
|
– |
Tensile Strength |
Yield Strength |
Elongation |
Hardness |
Hardness |
|
Grade |
(MPa) min |
0.2% Proof (MPa) min |
(% in 50mm) min |
Rockwell B (HR B) max |
Brinell (HB) max |
|
304 |
515 |
205 |
35 |
90 |
192 |
|
304L |
485 |
170 |
35 |
90 |
192 |
|
304H |
515 |
205 |
35 |
90 |
192 |
Grade specifications for 304L grade stainless steel
|
Grade |
UNS No |
Old British |
Euronorm |
Swedish SS |
Japanese JIS |
||
|
BS |
En |
No |
Name |
||||
|
304 |
S30400 |
304S31 |
58E |
1.4301 |
X5CrNi18-10 |
2332 |
SUS 304 |
|
304L |
S30403 |
304S11 |
- |
1.4306 |
X2CrNi19-11 |
2352 |
SUS 304L |
|
304H |
S30409 |
304S51 |
- |
1.4948 |
X6CrNi18-11 |
- |
- |
|
These comparisons are approximate only. The list is intended as a comparison of functionally similar materials not as a schedule of contractual equivalents. If exact equivalents are needed original specifications must be consulted. |
|||||||
Application
-
Heat Exchangers
-
Condensers
-
Off-Shore Oil Drilling Companies
-
Power Generation
-
Petrochemicals
-
Gas Processing
-
Specialty Chemicals
-
Chemical Equipment
-
Sea Water Equipment
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.