ASTM B462 UNS N08020 Superalloy Nickel Alloy Steel Pipe Flange B16.5

 

What is ASTM B462 UNS N08020?

Alloy 20 is often called as a superalloy. ASTM B462/ ASME SB462 UNS N08020 Flange has excellent resistance to general corrosion, pitting, and crevice corrosion in chemicals containing chlorides as well as in acidic medium or conditions that contain acidic solutions like sulfuric, phosphoric, and nitric acids.

 

Alloy 20 Flanges are a low-carbon containing, niobium-stabilized authentic alloy. Alloy 20 Flanges contain elements like nickel, iron, and chromium in their alloy with additions of metal elements like molybdenum and copper. The addition of niobium within the Alloy 20 Weld Neck Flange has been done to stabilize the alloy against sensitization and prevention of the resultant intergranular corrosion.

 

Features:

Corrosion resistant

Rust proof finish

Excellent stress distribution

Can sustain high pressure & temperature

 

Specification ASTM B462/ ASME SB 462 UNS N08020
Size 1/2" - 48"
Standards ANSI/ASME B16.5, B 16.47 Series A & B, B16.48, BS4504, BS 10, EN-1092, DIN, ANSI, ASME, BS, DIN, EN, GOST.
Class / Pressure 150#, 300#, 600#, 900#, 1500#, 2500#, PN6, PN10, PN16, PN25, PN40, PN64 etc
Main Types Forged / Threaded / Screwed / Plate
Types

Weld Neck Ring Flange (WNRF)

Slip-On Ring Flange (SORF)

Blind Ring Flange (BLRF)

Ring Type Joint Flange (RTJF)

Socket Weld Ring Flange (SWRF)

Lap Joint Ring Flange (LJRF)

 

 

Equivalent Grades:

STANDARD WERKSTOFF NR. UNS AFNOR EN
Alloy 20 2.4660 N08020 Z2NCUD31-20AZ NiCr20CuMo

 

Chemical Composition:

C Mn Si S Cu Ni Cr Fe Mo P
0.07 max 2 max 1 max 0.035 max 3-4 32-38 19-21 29.85 min 2-3 0.045 max

 

Mechanical Properties:

Density 8.1 g/cm3
Melting Point 1443 °C (2430 °F)
Tensile Strength Psi -80000, MPa - 551
Yield Strength (0.2%Offset) Psi - 35000, MPa - 241
Elongation 30 %

 

Applications:

Boiler & Heat Exchangers

Paper & Pulp Plants

High Pressure Applications

Oil and Gas Industries

Chemical Refinery

High Temperature Application

Water Pipe Line

Nuclear Power Plants

Food Processing Industries

 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Yuhong Group Co.,Ltd
Location 20TH FLOOR,NO.1 NEW WORLD BUILDING ,NO.1018 MINAN ROAD,YINZHOU DISTRICT, NINGBO CITY, ZHEJIANG PROVINCE, CHINA
Contact Person Jikin Cai

Request A Quote

Please check your email address.
Your message must be at least 20 characters.