EN12449 CuZn20Al2As C68700 Brass Seamless Tube for Power Plants Condenser
Price:
Negotiable
MOQ:
1000KGS
Delivery Time:
2-3 WEEKS
Brand:
YUHONG
Product Description
EN12449 CuZn20Al2As C68700 Brass Seamless Tube for Power Plants Condenser
Plant Condensers: Optimal Corrosion & Thermal Performance
- YUHONG Material: CuZn20Al2As (UNS C68700)
- YUHONG Standard: EN 12449:2018 Compliant
- YUHONG Application: High-Pressure Steam Condensers
- YUHONG Properties: Seawater Corrosion Resistance | Anti-Biofouling | High Thermal Conductivity
- YUHONG Certification: SCC Tested per EN ISO 196 (Ammonia Vapor)
EN12449 Chemical Compositions
| EN Designation | UNS Number | Alloy Name | Cu (+Ag) | Pb | Fe | Sn | Zn | Ni | Al | Mn | P | As | Sb | Other Elements | Cu + Sum Listed Elements |
| CW004A | C11000 | Copper | ≥99.90 | 0.005 | – | – | – | – | – | – | – | – | – | – | ≥99.97 |
| CW008A | C12000 | Phosphorus deoxidized Cu | ≥99.90 | 0.005 | – | – | – | – | – | – | 0.004–0.012 | – | – | – | ≥99.97 |
| CW024A | C21000 | Gilding brass | 94.0–96.0 | 0.05 | 0.05 | – | Rem. | – | – | – | – | – | – | – | ≥99.5 |
| CW502L | C22000 | Commercial bronze | 89.0–91.0 | 0.05 | 0.05 | – | Rem. | – | – | – | – | – | – | – | ≥99.5 |
| CW506L | C23000 | Red brass | 84.0–86.0 | 0.05 | 0.05 | – | Rem. | – | – | – | – | – | – | – | ≥99.5 |
| CW507L | C24000 | Low brass | 78.5–81.5 | 0.05 | 0.05 | – | Rem. | – | – | – | – | – | – | – | ≥99.5 |
| CW508L | C26000 | Cartridge brass | 68.5–71.5 | 0.07 | 0.05 | – | Rem. | – | – | – | – | – | – | – | ≥99.5 |
| CW600L | C31400 | Leaded commercial bronze | 87.0–89.0 | 0.7–1.2 | 0.1 | – | Rem. | – | – | – | – | – | – | – | ≥99.5 |
| CW602N | C31600 | Leaded brass | 85.0–87.0 | 0.7–1.2 | 0.1 | – | Rem. | – | – | – | – | – | – | – | ≥99.5 |
| CW614N | C33000 | Leaded brass | 65.0–68.0 | 0.25–0.7 | 0.07 | – | Rem. | – | – | – | – | – | – | – | ≥99.5 |
| CW617N | C33500 | Low-leaded brass | 62.0–65.0 | 0.25–0.7 | 0.15 | – | Rem. | – | – | – | – | – | – | – | ≥99.5 |
| CW702R | C68700 | Aluminum brass (CuZn20Al2) | 76.0–79.0 | 0.07 | 0.06 | – | Rem. | – | 1.8–2.5 | – | – | 0.02–0.10 | – | – | ≥99.5 |
| CW704R | C44300 | Admiralty brass | 70.0–73.0 | 0.07 | 0.06 | – | Rem. | – | – | – | – | 0.02–0.10 | 0.02–0.10 | – | ≥99.5 |
| CW706R | C44400 | Inhibited brass | 70.0–73.0 | 0.07 | 0.06 | – | Rem. | – | – | – | – | 0.02–0.10 | – | P: 0.02–0.10 | ≥99.5 |
| CW707R | C44500 | Inhibited brass | 70.0–73.0 | 0.07 | 0.06 | – | Rem. | – | – | – | 0.02–0.10 | – | – | – | ≥99.5 |
| CW712R | C46400 | Naval brass | 60.0–63.0 | 0.2 | 0.1 | 0.7–1.0 | Rem. | – | – | – | – | – | – | – | ≥99.5 |
| CW715N | C48600 | Leaded silicon brass | 87.0–90.0 | 0.7–1.4 | 0.2 | 1.3–2.2 | Rem. | – | – | – | – | – | – | Si: 0.5 max | ≥99.5 |
| CW721R | C70600 | CuNi10Fe | Rem. | 0.02 | 1.0–2.0 | – | – | 9.0–11.0 | – | 0.5–1.0 | – | – | – | Mn: 0.5–1.0 | ≥99.5 |
| CW725R | C71500 | CuNi30Fe | Rem. | 0.02 | 0.4–1.0 | – | – | 29.0–32.0 | – | 0.5–1.0 | – | – | – | Mn: 0.5–1.0 | ≥99.5 |
EN12449 Mechanical Properties
| EN Designation | UNS Number | Temper (TP) | Rₘ (MPa) min | Rp₀.₂ (MPa) min | A (%) min¹ | Hardness HBW max |
| CW004A | C11000 | O60 (Soft) | 200 | 40 | 43 | 45 |
| H110 (Hard) | 290 | 250 | 6 | 100 | ||
| CW008A | C12000 | O60 (Soft) | 200 | 40 | 43 | 45 |
| CW024A | C21000 | O60 (Soft) | 240 | 80 | 40 | 65 |
| CW502L | C22000 | O60 (Soft) | 270 | 80 | 42 | 65 |
| CW506L | C23000 | O60 (Soft) | 300 | 100 | 45 | 75 |
| CW507L | C24000 | O60 (Soft) | 330 | 110 | 45 | 80 |
| CW508L | C26000 | O60 (Soft) | 340 | 120 | 42 | 100 |
| H110 (Hard) | 500 | 420 | 10 | 150 | ||
| CW600L | C31400 | O50 (Light annealed) | 270 | 80 | 40 | 75 |
| CW602N | C31600 | O50 (Light annealed) | 270 | 80 | 40 | 75 |
| CW614N | C33000 | O50 (Light annealed) | 340 | 140 | 25 | 95 |
| CW617N | C33500 | O50 (Light annealed) | 340 | 140 | 25 | 95 |
| CW702R | C68700 | O50 (Light annealed) | 450 | 180 | 25 | 130 |
| H110 (Hard) | 650 | 550 | 8 | 210 | ||
| CW704R | C44300 | O60 (Soft) | 340 | 120 | 45 | 100 |
| CW706R | C44400 | O60 (Soft) | 340 | 120 | 45 | 100 |
| CW707R | C44500 | O60 (Soft) | 340 | 120 | 45 | 100 |
| CW712R | C46400 | O60 (Soft) | 380 | 170 | 35 | 115 |
| H110 (Hard) | 550 | 450 | 12 | 200 | ||
| CW715N | C48600 | O50 (Light annealed) | 340 | 140 | 25 | 95 |
| CW721R | C70600 | O50 (Light annealed) | 340 | 120 | 30 | 90 |
| CW725R | C71500 | O50 (Light annealed) | 370 | 120 | 30 | 100 |
EN12449 Supplementary Requirements (All Grades)
| Property | Test Method | Requirement |
| Hydrostatic Test | EN ISO 10896 | Min. pressure: 6 MPa (60 bar) for ≥10 sec; no leakage or deformation |
| Flare Test | EN ISO 8494 | Expand to 25% of OD without cracking (for tubes ≤100mm OD in soft temper) |
| Grain Size (Soft Tubes) | ASTM E112 / ISO 2624 | Min. grain size 0.020 mm (ASTM 6.0) for O60/O50 tempers |
| Stress Corrosion (SCC) | EN ISO 196 / ISO 6957 | Optional: Pass ammonia vapor test (7 days, 35% NH₄OH) for brass alloys |
| Dezincification Resistance² | ISO 6509 | For brass alloys: Max. depth 100 µm (Class B/C requirements vary per alloy) |
Related Videos
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.
Company
Yuhong Group Co.,Ltd
Location
20TH FLOOR,NO.1 NEW WORLD BUILDING ,NO.1018 MINAN ROAD,YINZHOU DISTRICT, NINGBO CITY, ZHEJIANG PROVINCE, CHINA
Contact Person
Jikin Cai