High Purty 99.6% Ni200 Ni201 Ni212 Pure Nickel N4 N6 Precision Stranded Alloy Wire for Power Tools Machinery
Commercially wrought Nickel 200 ( UNS N02200) , a grade of pure nickel contains 99.2% nickel, has excellent mechanical properties, magnetic properties, high thermal, electrical conductivity and excellent resistance to many corrosive environment. Nickel 200 is useful in any environment below 600ºF(315ºC). It has highly resistance to neutral and alkaline salt solutions. Nickel 200 also has low corrosion rates in neutral and distilled water.
The applications of pure nickel includes food processing equipment, magnetostrictive devices and rechargeable batteries, computers, cellular Phone, power tools, camcorders and so on.
| Density | 8.89g/cm3 |
| Specific Heat | 0.109(456 J/kg.ºC) |
| Electrical Resistivity | 0.096×10-6ohm.m |
| Melting Point | 1435-1446ºC |
| Thermal Conductivity | 70.2 W/m-K |
| Mean Coeff Thermal Expansion | 13.3×10-6m/m.ºC |
Chemical Composition
| Nickel Grade | Ni+Co | Cu | Si | Mn | C | Cr | S | Fe | Mg |
| ≥ | ≤ | ||||||||
| Ni201 | Bal. | .25 | .3 | .35 | .02 | .2 | .01 | .3 | - |
| Ni200 | Bal. | .25 | .3 | .35 | .15 | .2 | .01 | .3 | - |
| Alloy | Standard Strand Construction, mm | Resistance,Ω/m | Strand Diameter Nominal, mm | Meter per Kilo |
| NiCr 80/20 | 18×0.544+1x0.574 | 0.252-0.278 | 2.67 | 26 |
| NiCr 80/20 | 19×0.61 | 0.205-0.250 | 3.05 | |
| NiCr 80/20 | 18×0.523+1x0.574 | 0.271-0.299 | 2.67 | 30 |
| NiCr 80/20 | 19×0.574 | 0.227-0.251 | 2.87 | 25 |
| NiCr 80/20 | 36×0.385+1x0.45 | 0.265-0.293 | 2.76 | 26 |
| NiCr 60/15 | 19×0.508 | 0.286-0.318 | 2.54 | |
| NiCr 60/15 | 18×0.523+1x0.574 | 0.276-0.305 | 2.76 | 30 |
| Ni200/Ni201 | 19×0.574 | 0.019-0.021 | 2.87 | 21 |
| Propertes/Grade | Cr20Ni80 | Cr30Ni70 | Cr15Ni60 | Cr20Ni35 | Cr20Ni30 | |
| Main Chemical composition | Ni | Rest | Rest | 55.0-61.0 | 34.0-37.0 | 30.0-34.0 |
| Cr | 20.0-23.0 | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 18.0-21.0 | |
| Fe | ≤ 1.0 | ≤ 1.0 | Rest | Rest | Rest | |
| Max. continuous service temp. of element | 1200 | 1250 | 1150 | 1100 | 1100 | |
| Resistivity at 20oC (μ Ω · m) | 1.09 | 1.18 | 1.12 | 1.04 | 1.04 | |
| Density (g/cm3) | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 | |
| Thermal conductivity(KJ/m· h· oC) | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 | |
| Coefficient of lines expansion(α × 10-6/oC) | 18 | 17 | 17 | 19 | 19 | |
| Melting point (approx. )( oC) | 1400 | 1380 | 1390 | 1390 | 1390 | |
| Elongation at rupture (%) | > 20 | > 20 | > 20 | > 20 | > 20 | |
| Micrographic structure | austenite | austenite | austenite | austenite | austenite | |
| Magnetic properties | nonmagnetic | nonmagnetic | nonmagnetic | nonmagnetic | nonmagnetic | |