High Purity Scandium Metal Applied In Various Superalloys

Price Negotiable
Price: TBA
MOQ: 100g
Delivery Time: About 7 days
Brand: High Broad
Product Description

High Purity Scandium Metal Applied In Various Superalloys

 

High Broad is able to supply scandium metal in purities from 99.5% to 99.999%, as well as scandium oxide (Sc2O3) in purities from 99.99% min. Please contact us with your specific requirement or for a current scandium price.

 

Scandium is a very light elemental metal that is often found alongside the rare earth elements. Due to it's rarity and high price, scandium does not have a lot of commercial applications, but is used in specialty halide lamps, as well as lightweight, high-strength alloys. It is estimated that only as little as a couple hundred kilograms of scandium metal are produced each year.

 

Chemical Formula: Sc
Description: Light, silvery-grey metal
Purity: TREM 99-99.95%, Sc/TREM 99.9% min.
Packing: As required
CAS No: 7440-20-2

 

RE Element Max. Impurity (ppm) Element Max Impurity (ppm)
La 4.5 Mn 9.3
Ce 7.3 Fe 20.8
Pr 3.5 Si 10.2
Nd 6.9 Ca 9.9
Sm 4.3 Mg 1.3
Eu 1.9 Cu 9.4
Gd 8.3 Ni 5.7
Tb 4.4 Al 34.9
Dy 5.9 Zn 4.0
Ho 8.2 Ti 35.2
Er 5.5 Ag 1.6
Tm 6.3 Cd 0.8
Yb 2.0 O 280

 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Hunan High Broad New Material Co.Ltd.
Location 70 Chezhan North Road, Changsha,China
Contact Person Vivian Jiang

Request A Quote

Please check your email address.
Your message must be at least 20 characters.