Three Side Seal Package Leak Tester 0-600 KPa Burst Creep Test
Price:
Get An Offer
MOQ:
1 SET
Delivery Time:
3~5 days
Brand:
Cell Instruments
Product Description
Three Side Seal Package Leak Tester conforms to standards of ISO 11607-1, ISO 11607-2, ASTM F1140, ASTM F2054, GB/T 10440, GB 18454, GB 19741, GB 17447, GB/T 17876, GB/T 10004, BB/T 0025, QB/T 1871, YBB 00252005, YBB 00162002 .
Principle
The three test modes of the positive pressure method
- Burst Test: It internally pressurizes the packages until the package fails. The test pressure is the maximum pressure detected before the package fails.
- Creep Test: Pressurize the package internally to a specific pressure and maintains this pressure for a specific time. The test measure is pass/fail.
- Creep to Failure: The package is creep-tested and held until the package fails. The pressure setting is higher than that of the creep test to ensure the package fails in some time. The measure is the time until failure.
Features
- Three test modes of burst, creep and creep to failure are available.
- PLC programmable logic controller realizes precise pressure and time control.
- 7 inch TFT touching screen for convenient parameter setting and test operation.
- Multiple groups of test parameters can be save to avoid the repetitive setting time.
- Test result auto statistics and storage.
- Program customization available.
Three Side Seal Package Leak Tester Technical Specifications
Pressure Range 0 ~ 600 KPa; 0 ~ 87.0 psi (Standard)
Inflating Head Φ4mm (Standard)
Gas Pressure 0.4 MPa~0.9 MPa
Port Size Φ6 mm PU hose
Dimensions 400 mm (L) × 270 mm (W) × 180 mm (H)
Pedestal Size 375 mm (L) × 275 mm (W) × 345 mm (H)
Similar Products
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.
Company
Cell Instruments Co., Ltd.
Location
1-403,Bldg 4-B-1,No. 5577 Gongyebei Rd, Licheng District, Jinan, 250109, Shandong, China
Contact Person
Owen Zhang