Differential Scanning Calorimetry Machine Providing Detailed Temperature and Gas Flow Settings with Touch Screen Interface
Advanced DSC analyzer with touch-screen interface, specifically designed for determining oxidation induction time (OIT) of polymeric materials. Features one-touch operation and fully automated software-controlled testing procedures.
This instrument complies with the following national and international standards:
- GB/T 19466.2-2009 / ISO 11357-2:1999
- GB/T 19466.3-2009 / ISO 11357-3:1999
- GB/T 19466.6-2009 / ISO 11357-6:1999
- Industrial-grade widescreen touch interface with comprehensive real-time data display
- USB communication interface with high universality and stable data transmission
- Compact furnace chamber structure with adjustable heating and cooling rates
- Optimized mechanical fixation installation eliminating interference
- Electric heating with compressor-driven circulating cooling water system
- Dual temperature probes for high repeatability in temperature measurement
- Automatic two-channel gas switching with fast response
- Standard reference samples for convenient calibration
- Software compatible with all screen resolutions and Windows operating systems
- Customizable device operation modes for automated measurement sequences
- Fully enclosed support structure reducing contamination and maintenance
| Temperature range | 0℃~500℃ |
| Temperature resolution | 0.01℃ |
| Heating rate | 0.1~40℃/min |
| Cooling rate | 0.1~20℃/min |
| Calorimetric resolution | 100% |
| Constant temperature | 5℃~500℃ |
| Temperature control mode | Heating, cooling, constant temperature |
| DSC range | 0~±500mW |
| DSC resolution | 0.01mW |
| Working power | AC 220V 50Hz 300W or other |
| Atmosphere control gas | Two-channel automatic control (nitrogen and oxygen) |
| Gas flow | 0-200mL/min |
| Gas flow accuracy | 0.2mL/min |
| Crucible | Aluminium crucible Φ6.6*3mm |
| Display mode | 7-inch touch screen |
| DSC machine | 1 set |
| Aluminium crucibles | 300 pieces |
| Power cords and USB cable | Each one |
| CD (software and operations video) | One |
| Oxygen airway and nitrogen airway | Each 5m |
| Standard samples (indium, tin, zinc) | Each one |
| External circulation thermostat sink | One |
The temperature control range covers from ambient temperature to 600℃, with a temperature measurement accuracy of ±0.1℃ and temperature repeatability error less than 0.05℃, ensured by dual temperature probes and proprietary temperature control technology.
The heating rate is adjustable from 0.1℃/min to 99.9℃/min, and the cooling rate ranges from 0.1℃/min to 50℃/min (supported by compressor-driven circulating cooling water), meeting diverse test rate requirements.
It is equipped with a dual-channel gas automatic switching system (oxygen and nitrogen), with a flow adjustment range of 0-500 mL/min and a switching stabilization time of less than 10 seconds, ensuring stable and accurate gas supply during oxidation induction period tests.