Inconel 718 Nickel Alloy Tube 965 MPa Tensile Strength Stress Corrosion Cracking Resistance

Price Negotiable
Price: FobShanghai usd 5.9-6.4/kg
MOQ: 100kgs
Delivery Time: 25-30 days subject to the clients' requirement and quantity
Brand: BLM-DX-1
Product Description

Inconel 718

Inconel 718 Chemical composition

 

Alloy % Ni Cr Fe Mo Nb Co C Mn Si S Cu Al Ti
718 Min. 50 17 balance 2.8 4.75             0.2 0.7
Max. 55 21 3.3 5.5 1 0.08 0.35 0.35 0.01 0.3 0.8 1.15

 

 

Inconel 718 Physical properties

 

Density 8.2 g/cm³
Melting point 1260-1340 ℃

 

 

Inconel 718 Alloy minimum mechanical properties in the roomtemperature

 

Alloy Tensile strength Rm N/mm² Yield strength R P0. 2N/mm² Elongation A 5 %

Brinell hardness

HB

Solution treatment 965 550 30 ≤363

 

 

718 Characteristic as below:

1.workability

2.High tensile strength,endurance strength,creep strength and rupture strength at 700℃.

3.High inoxidability at1000℃. 4.Steady mechanical performance in the low temperature.

5.Good welding performance.

 

 

Inconel 718 Metallurgical structure

 

718alloy is Austenitic structure, precipitation hardening generate "γ" made it excellent mechanical performance. G rain boundary generate "δ" made it the best plasticity in the heat treatment.

 

 

 

Inconel 718 Corrosion resistance

 

718 alloy with extremely resistance to stress corrosion cracking and pitting ability in high temperature or low temperature environments, especially the inoxidability in the high temperature.

 

 

Inconel 718 Application field:

1 . The elevated temperature strength, excellent corrosion resistance and workability at 700℃ properties

2 . made it use in a wide range of high requirement environments :Steam turbine ; Liquid-fuel rocket ; Cryogenic engineering

3.Acid environment

4.Nuclear engineering

 

 

 

 

 

 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company BLOOM(suzhou) Materials Co.,Ltd
Location B615, Future Fortune Building, No. 1 Wangxi Road, Zhangjiagang City, Jiangsu Province
Contact Person Kara Liu

Request A Quote

Please check your email address.
Your message must be at least 20 characters.