Medical Grade Platinum Silicone Rubber Ozone Resistance Liquid Silicone Rubber Tube
Medical Grade Platinum Silicone Rubber Ozone Resistance Liquid Silicone Rubber Tube
Description
LSR RH6250-40YH is food grade liquid silicone rubber for injection molding processes. At higher temperatures the safety operation time shortened. LSR RH6250-40YH liquid silicone rubber is platinum cured(vulcanized) materials which are mixed in a 1:1 ratio by weight. This product is suitable for the two-component injection molding process. LSR is platinum cured(vulcanized) materials which are mixed in a 1:1 ratio by weight.
Typical Properties
| LSR- RH6250 - 40YH | |||
| Properties | Unit | A | B |
| Appearance | / | transparent | transparent |
| Viscosity | mPa.s | 1400000-2000000 | |
| Density | g/cm3 | 1.10±0.02 | |
| Shore A Hardness | A/JLS | 40±3 | |
| Tensile Strength | MPa | ≥7.5 | |
| Elongation at break | % | ≥550 | |
| Tear Strength | KN/m | ≥20 | |
| Linear Shrinkage | % | ≤0.1 | |
| Tensile set | % | ≥1.7 | |
| Rebound | % | ≥55 | |
| Compression set | (22 hrs at 175℃) % | ≤35 | |
These figures are for reference only, please contact us for details.
Typical properties of the vulcanisate:
The mixing ratio of components A: B = 1: 1.
Applications
Because of the outstanding properties, LSR RH6250-40YH Lquid silicone rubber is particularly suitable for the following elastomeric articles: medical sacculus, negative pressure ball, catheter connector, sealing elements, diaphragms, ear plugs, bellows, baby teats, respiratory devices, air vent flaps, tube connectors, catheters, parts for medical technical equipment, mat, etc.
Certificate
Rui-He RH6250-40YH Liquid silicone rubber obtained the following test certificate: RoHS, FDA, MSDS, LFGB, ISO9001:2016.
Packaging & Storage
- LSR-RH6250-40YH Medical is available in 20kgs pails or 200kgs drums.
- Store in a cool dry place out of direct sunlight, use it within 12 months from the day of manufacture.
Notice
This product cannot be contacted with compounds containing N, P, S to avoid affecting the catalytic effect of platinum.
FAQ
Q: Why is the tear strength of the silicone mold weak?
A: There are three reasons:
- In order to reduce the viscosity of silicone rubber and pursue a good quality, you may add a lot of silicone oil into the silicon rubber when making molds. In fact, it might have just the opposite effect. The tension and the tear strength will be reduced badly with the addition of silicon oil. And the silicon molds will be in a weak and flimsy manner.
- You may add too much catalyst into the silicone rubber, we suggest customers add catalyst no more than 5%, 2%will be perfect.
- You may use the silicone mold too early after it finished. We suggest the customer begin using the molds after 24 hours. What’s more, it will be better if you can make an outer mold to protect the silicone mold.
Why Choose Us?
1. 15 years of manufacturing experience focus on silicone rubber
2. All Products shipped is Up to FDA, Rosh, Reach, LFGB, testing standard
3. Overall quality controlling procedure and perfect service to you
4. Offer to tailor the order accordance with customer's requirement in detail.
5. 800 tons solid silicone rubber, 300 tons LSR silicone rubber and 200 tons silicone oil every month
6. Special organic silicon R&D team and precision inspection instruments equiped
7. Automatic manufacturing equipment adopted, which ensure the products shipped quality well largely
If you need to know the prices of our silicone rubbers, please contact us. We do not provide prices on the website because prices fluctuate for many reasons.
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.