hefei fuyun environmental sci-tech co.,ltd.
                                                                                                           
Verified Supplier
7 Years
Since 2019
Menu

Environmental Geomembrane Fabric Oxygenation HDPE 1.0mm Thickness

Price Negotiable
Price: USD 0.85-2.55 square meters
MOQ: 2000 square meters
Delivery Time: 10Days
Brand: FUYUN
Product Description

Lobster Tank Lining Environmental Geomembrane Fabric Oxygenation HDPE 1.0mm Thickness

 

Quick Detail:

  • material: HDPE, LDPE
  • length: 100m
  • width: 6m 
  • thickness:  1.0mm 
  • function: anti seepage, oxygenation, temperature control
  • application: fish pond, fish tank, shrimp tank, shrimp tank

Production Description:

 

Geomembrane liners remain the optimal choice for various aquaculture applications. With its excellent impermeability it allows for exceptional durability, high chemical & UV resistance and offering superior weldability whilst being flexible enough to allow for ease of installation without compromising its integrity.

 

Environmental geomembrane is a kind of HDPE geomembrane, which is mainly made of opaque and translucent thermoplastic resin material – polyethylene resin. High quality environmental geomembrane (wholesale environmental geomembrane) produced by the environmental high quality environmental geomembrane manufacturers is a high molecular polymer, which is a non-toxic, odorless and odorless white particle. It’s melting point is about 110-130℃, and its relative density is 0.918-0.965. The environmental high quality environmental geomembrane produced by the environmental geomembrane manufacturers (environmental geomembrane factory price) has good heat resistance and cold resistance. It has good chemical stability, high rigidity, and toughness, good mechanical strength, good resistance to environmental stress cracking and tear strength. With the increase in density, mechanical properties and barrier properties will be correspondingly improved, heat resistance and tensile strength will be higher; it can resist acid, alkali, organic solvents and other corrosion.

 

Table1(a) – High Density Polyethylene (HDPE) Geomembrane -Smooth

 

 

  Properties Test       Test Value       Testing Frequency
    Method 30 mils 40 mils 50 mils   60 mils 80 mils 100 mils 120 mils (minimum)
Thickness (min. ave.) D5199 nom. Nom. Nom.   Nom. Nom. Nom. Nom. Per roll
· lowest individual of 10 values   -10% -10% -10%   -10% -10% -10% -10%  
Density mg/l (min.) D 1505/D 792 0.940 g/cc 0.940 g/cc 0.940 g/cc   0.940 g/cc 0.940 g/cc 0.940 g/cc 0.940 g/cc 200,000 lb
Tensile Properties (1) (min. ave.) D 6693                 20,000 lb
· yield strength Type IV 63 lb/in. 84 lb/in. 105 lb/in.   126 lb/in. 168 lb/in. 210 lb/in. 252 lb/in.  
· break strength   114 lb/in. 152 lb/in. 190 lb/in.   228 lb/in. 304 lb/in. 380 lb/in. 456 lb/in.  
· yield elongation   12% 12% 12%   12% 12% 12% 12%  
· break elongation   700% 700% 700%   700% 700% 700% 700%  
Tear Resistance (min. ave.) D 1004 21 lb 28 lb 35 lb   42 lb 56 lb 70 lb 84 lb 45,000 lb
Puncture Resistance (min. ave.) D 4833 54 lb 72 lb 90 lb   108 lb 144 lb 180 lb 216 lb 45,000 lb
Stress Crack Resistance (2) D5397 300 hr. 300 hr. 300 hr.   300 hr. 300 hr. 300 hr. 300 hr. per GRI-GM10
    (App.)                  
Carbon Black Content (range) D 4218 (3) 2.0-3.0% 2.0-3.0% 2.0-3.0%   2.0-3.0% 2.0-3.0% 2.0-3.0% 2.0-3.0% 20,000 lb
Carbon Black Dispersion D 5596 note (4) note (4) note (4)   note (4) note (4) note (4) note (4) 45,000 lb
Oxidative Induction Time (OIT) (min. ave.) (5)                   200,000 lb
(a) Standard OIT D 3895 100 min. 100 min. 100 min.   100 min. 100 min. 100 min. 100 min.  
  — or —                    
(b) High Pressure OIT D 5885 400 min. 400 min. 400 min.   400 min. 400 min. 400 min. 400 min.  
Oven Aging at 85°C (5), (6) D 5721                  
(a) Standard OIT (min. ave.) - % retained after 90 days D 3895 55% 55% 55%   55% 55% 55% 55% per each
  — or —                   formulation
(b) High Pressure OIT (min. ave.) - % retained after 90 days D 5885 80% 80% 80%   80% 80% 80% 80%  
UV Resistance (7) D 7238                  
(a) Standard OIT (min. ave.) D 3895 N.R. (8) N.R. (8) N.R. (8)   N.R. (8) N.R. (8) N.R. (8) N.R. (8) per each
  — or —                   formulation
(b) High Pressure OIT (min. ave.) - % retained after 1600 hrs (9) D 5885 50% 50% 50%   50% 50% 50% 50%  

 

Specification:

 

general parameter:

Thickness 0.15-3.0mm & customer ' s requirement
Width 1-8m & customer ' s requirement
Length 50-200m & customer ' s requirement
Material HDPE
Color Black,White,Green,Blue & customer ' s requirement
Surface Smooth
Package Double layers woven bag, and add two strap & customer ' s requirement
Shipping Marks support
Production Standard GRI,ASTM,GB or other standard

 

specific parameter:

Item Properties Unit Thickness
1 Thickness mm 0.25 0.35 0.5 0.75 1 1.25 1.5 2
2 Density g/m3 0.94
3 Stretch Yield Strength (horiz & vet) N/mm 3.75 5 7.5 11 15 18 22 29
4 Stretch Break Strength (horiz & vet) N/mm 6.75 13.5 19 20 27 33 40 53
5 Yield Elongation (horiz & vet) % 12
6 Break elongation (horiz & vet) % 700
7 Angle Tear Strength (horiz & vet) N 31.25 45 62.5 93 125 156 187 249
8 Puncture Strength N 80 150 160 240 320 400 480 640
9 Stress Crack Resistance Hrs 300
10 Carbon Black Content (range) % 2.0-3.0
11 Carbon Black Dispersion / not more than 1 case grade 3 in 10 samples, grade 4 & 5 is not allowed
12 Oxidation Induction Time(OIT) Standard OIT 100 min
High Pressure OIT 400 min
13 Thermal Aging at 85 Standard OIT(min.ave.) retained after 90 days 55%
High Pressure OIT(min.ave.) retained after 90 days 80%
14 UV Resistance Standard OIT (min.ave.) 50%
High Pressure OIT (min.ave.) retained after 1600 hrs 50%
       

 

 

Application:

 

1, Aquaculture: factory breeding pool, fish pond, shrimp ponds circle of lining, sea cucumber, slope protection, etc.;

 

 

Advantage:

  • High anti-seepage ratio
  • Chemical stability
  • Anti plant root system
  • Thermal aging resistance
  • High mechanic strength
  • Low cost
  • Environmental protection formulation
  • Rapid construction

Package:

 

Packaging Details:

Neutral package of Pond Liner Material

Roll Size: 4m-7.0m

Or packed according to customers' requirements such as mark the company Logo

As example:

Specification 20ft container 40ft container

0.5mm 5.8/7*420m/roll 16rolls/38976m2 19rolls/55860m2

0.75mm 5.8/7*280m/roll 16rolls/25984m2 19rolls/37240m2

1mm 5.8/7*210m/roll 16rolls/19488m2 19rolls/27930m2

1.5mm 5.8/7*140m/roll 16rolls/12992m2 19rolls/18620m2

2.0mm 5.8/7*105m/roll 16rolls/9744m2 19rolls/13965m2

 

Factory Show:

 

 

 

Why Choose us?

 

 

FAQ:

 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company hefei fuyun environmental sci-tech co.,ltd.
Location Building 3, No.55 Science Avenue, High Tech Zone, Hefei, Anhui, China
Contact Person Jenny

Request A Quote

Please check your email address.
Your message must be at least 20 characters.