S20430 Stainless Steel Spring Wire
ASTM A313 UNS S20430 Stainless Steel Spring Wire
S20430 is a chromium-magnesium austenitic stainless steel with an addition of 2-4% copper and nitrogen of 0.05-0.25%. Due to the addition of copper the alloy has better formability than 201 and 304. The copper improves corrosion and resistance to stress corrosion cracking in certain media.
Chemical composition
| C | Si | Mn | Ni | P | S | Cr | N | Cu |
| max 0.15 | max 1 | 6.5-9.0 | 1.5-3.5 | max 0.060 | max 0.030 | 15.5 - 17.5 | 0.05-0.25 | 1.50-2.50 |
Specification
ASTM A313M-2003 Stainless Spring Steel Wires
Supplying Size
Diameter 0.1 to 15 mm ; 0.005 to 0.6 inch
Delivery condition
Types S20430 shall be cold drawn to produce the required mechanical properties.
Surface condition
Stainless steel spring wire is supplied with different types of finish such as bright, copper, lead, oxide, and other.
Tensile Strength
Application
Stainless steel wire is the raw material for screws, springs, metallic net, cable wire and hardware. It is widely used in filter, building and important for electronic parts, oil and fiber industry, kitchenware and hardware.
Mill test certificate
EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.