T-Shirt Heat Transfer Printing TPU DTF Powder Hot Melt White Adhesive Powder
T-Shirt Heat Transfer Printing TPU DTF Powder Hot Melt White Adhesive Powder
Adhesive and Bonding:
Strong Adhesion: TPU powder offers robust adhesive properties, ensuring a secure bond between the design on the transfer film and the substrate during the heat transfer process.
Durable Bond: The TPU powder creates a durable bond that is resistant to washing and wear, maintaining the integrity of the design over time.
Flexibility and Elasticity:
Flexibility: TPU is known for its flexibility and elasticity, allowing the transferred design to retain its stretch and shape properties, making it suitable for fabrics that require some degree of stretch.
Crease Resistance: TPU powder helps the design resist creases and wrinkles, ensuring a smooth and uniform appearance even after wear and washing.
Compatibility and Applications:
Versatile Substrates: TPU DTF powder is compatible with a wide range of substrates, including cotton, polyester, and blends, making it suitable for diverse textile printing applications.
Textile Printing: It is frequently used in textile printing for creating custom designs on clothing, textiles, and accessories with vibrant colors and intricate details.
Product model: ES221
Description: Polyurethane hot melt adhesive powder
Function:Heat transfer,Digital printing,Silk screen printing.
Physical Characteristics:
| Property | Criterion |
| Appearance | White powder |
| Composition | TPU |
| Density ASTM D-792 | 1.2±0.02g/cm³ |
| Melt Point DSC | 110-125 ℃ |
| Melt Index ASTM D-123825 | 25±8g/10min |
| Powder size range | 0-80 um |
| 80-170 um | |
| 80-200 um | |
| 100-200 um |
Technical Parameters:
| Bonding parameters (for reference only) | Temperature | 130-170℃ |
| Press | 3.0 kg/cm2 | |
| Time | 14S | |
| Washing Resistance | 40℃ | Excellent |
| 60℃ | good | |
| 90℃ | / |
Packaging and Storage Conditions:
| Packaging | 20KG in one PE bag+Brown paper bag |
| Storage Conditions | Stored in dry unopened packaging at room temperature for 12 months. High temperature and pressure will cause agglomeration. The trays cannot be double-pressed. |
1. Bonding temperature and pressure and time relate to the bonding strength of the film to the material. The bonding temperature must be close to the temperature set by the machine, the pressure must be uniform, and the mold and press rolls must be flat.