Alloy 901 / 2.4975 is a nickel-chromium-molybdenum alloy containing titanium.
Size Range
Round bar / Wire rod (Diameter): 8.0 mm to 1000 mm
Square bar / Flat bar: 8.0 mm to 1000 mm
Forging piece: Stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
Heavy/middle plate via hot rolled: T5 - 200 mm X W10 - 1000 mm X L1000-12000 mm
Sheet steel via cold rolled: T5 - 10 mm X W5 - 1000 mm X L1000 - 1000 mm
Steel strip via cold rolled: T0.5 - 8.0 mm X W10 - 200 mm X L (or in coil form)
Length: Fixed length or random length or based on the customer's special requirement.
Chemical Composition and standard
|
Incoloy 901/N90901/AISI 682 |
NiFeCr12Mo/2.4975 | AMS 5660 |
| ASTM Udimet 901 | DIN EN 10095-2018 | SAE AMS 5660L-2015 |
|
Mo(%): 5.30~6.50 Ti(%): 2.20~2.75 B(%): 0.01~0.02 Al(%): ≤0.35 Cu(%): ≤0.50 Fe(%): Remainder
|
C(%): ≤0.10 Mo(%): 5.0~7.0 Ti(%): 2.35~3.1 Co(%): ≤1.0 Al(%): ≤0.35 Fe(%): Remainder |
C(%): ≤0.10 Mo(%): 5.0~7.0 Ti(%): 2.35~3.10 B(%): 0.01~0.02 Co(%): ≤1.0 Al(%): ≤0.35 Cu(%): ≤0.50 Pd(%): ≤5 ppm Bi(%): ≤0.3 ppm Se(%): ≤3 ppm Fe(%): Remainder
|
Mechanical Properties
Tensile strength, σb/Mpa: ≥175
Yield Point, σs/Mpa: ≥ 125
Elongation, δ/%: 15
Reduction of Area,ψ/%: ≥19
Applications
- aviation industry
- ship industry
- Industrial Sector Gas Turbines
Contact us
If you are interested in our products or have any questions, please contact our team of engineers at
sales@ss-bars.com
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.