Mianyang Baoheng New Material Technology Co.,Ltd
                                                                                                           
Verified Supplier
Years
Since
Menu

Udimet 710 Superalloy Hot Rolled Strips ATG W4 Sheet Steel 0.3-8mm Thickness

Price Negotiable
Price: Negotiations
MOQ: 600kg
Delivery Time: Ex-stock for delivery: 3-7 days Production lead time: 30-60 days
Brand: PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Product Description

Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips


 
Product Information

 

Udimet 710 superalloy has good oxidation resistance and creep resistance, and can be strengthened by precipitation hardening, solution hardening and work hardening. They also function under high mechanical stress and high temperature and where high surface stability is required


Size Range
 
Round bar / Wire rod (Diameter): 1.0 mm to 500 mm
Square bar / Flat bar: 1.0 mm to 500 mm
Forging piece: Stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
Heavy/middle plate via hot rolled: T3 - 1000 mm X W8 - 1000 mm X L800-12000 mm
Sheet steel via cold rolled: T5.0 - 8 mm X W5 - 1000 mm X L100 - 1000 mm
Steel strip via cold rolled: T0.3 - 8 mm X W10 - 1000 mm X L (or in coil form)
Length: Fixed length or random length or based on the customer's special requirement.
 
 
Chemical Composition and standard

 

 
Udimet 710
 

ATG W4

ASTM A959(2004)

JIS G4303(2005)


C(%): ≤0.07
Si(%): -
Mn(%): -
P(%)≤: -
S(%)≤: -
Cr(%):
≤18.0
Ni(%): ≤55.0
Mo(%): ≤3.0

W(%): ≤1.50

Al(%): ≤2.50

Ti(%): ≤5.0

Fe(%): ≤0.50

Co(%): ≤14.8

B(%): ≤0.02

 

C(%): ≤0.07
Si(%): -
Mn(%): -
P(%)≤: -
S(%)≤: -
Cr(%):
≤18.0
Ni(%): Remainder
Mo(%): ≤3.0

W(%): ≤1.50

Al(%): ≤2.50

Ti(%): ≤5.0

Fe(%): -

Co(%): -

B(%): ≤0.02

 


 
X120Mn12/1.3401 Mechanical Properties

 

Tensile strength, Rm/MPa: -
Yield strength, Rp/MPa: -
Elongation/%: -
Reduction of area, ψ/%: --

Impact, KV /J: -
Hardness, HBW: --

 
Applications

Udimet 710 is suitable for various high-temperature environments, such as steam and gas turbines.

 

If you are interested in our products or have any questions, please contact our team of engineers at
sales@ss-bars.com

 

 
 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Mianyang Baoheng New Material Technology Co.,Ltd
Location Building 4A, Cross-border E-commerce Industrial Park, Shiqiaopu, High-tech Zone, Mianyang City, SC, China
Contact Person Bruce Chiu

Request A Quote

Please check your email address.
Your message must be at least 20 characters.