Hot Rolled Peeled Superalloy Round Rod ASTM N155 UNS R30155 5.5mm-800mm
ASTM N155 UNS R30155 Alloy Round Bar ASTM N155 Superalloy Round Bar UNS R30155 Bar
Description
Our company provides ASTM N155 Solution treated Bar UNS R30155 Quenched and Tempered Alloy Round Bar ASTM N155 Superalloy Peeled Round Bar UNS R30155 Machined Bar.
All of ASTM N155 Solution treated Bar UNS R30155 Quenched and Tempered Alloy Round Bar ASTM N155 Superalloy Peeled Round Bar UNS R30155 Machined Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.
- Material:Metal,ASTM N155 UNS R30155 Alloy Round Bar ASTM N155 Superalloy Round Bar UNS R30155 Bar
- Shape:Superalloy Round Bar
-
Round bar / Wire rod (Diameter): 5.5mm to 800mm
-
Square bar / Flat bar: 3mm to 800mm
-
Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm
-
Sheet steel via cold rolled: T0.5 - 6mm X W6 - 1000mm X L1000 - 2000mm
-
Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)
Products Details
ASTM N155 Solution treated Bar UNS R30155 Quenched and Tempered Alloy Round Bar ASTM N155 Superalloy Peeled Round Bar UNS R30155 Machined Bar.
| Chemical Composition (weight%): | |
| C | 0.08 ~ 0.16 |
| Cr | 20.0 ~ 22.5 |
| Ni | 19.0 ~ 21.0 |
| Mo | 2.50 ~ 3.50 |
| W | 2.00 ~ 3.00 |
| Al | - |
| Ti | - |
| Fe | Remainder |
| Si | ≤ 1.00 |
| Mn | ≤ 1.00 |
| Other |
Nb: 0.75~1.25, Co : 18.0~21.0, P: ≤ 0.040,S: ≤ 0.030,N: ≤0.20 |
| Mechanical Properties Under Final Heat Treatment: | |
| Condition / Bar | Solution treated |
| Tensile strength, σb/≥ MPa | 690 ~ 930 |
| Yield strength, σ0.2/≥ MPa | 345 |
| Elonghation, δ ≥(%) | 20.0 |
| Reduction of area, ф ≥ (%) | - |
| Hardness | HB | - |
Applications:
ASTM N155 Solution treated Bar UNS R30155 Quenched and Tempered Alloy Round Bar ASTM N155 Superalloy Peeled Round Bar UNS R30155 Machined Bar.
Bolt and nut,Chemical equipment,Mechanical parts used in the condition of corrosion resistance,Pressure vessel.
Equivalent Grade
ASTM B639
ASTM N155
UNS R30155
ASTM N155 Solution treated Bar UNS R30155 Quenched and Tempered Alloy Round Bar ASTM N155 Superalloy Peeled Round Bar UNS R30155 Machined Bar.
FAQ
Q: How do you control the quality?
A: We have professional inspectors to analyze the chemical composition of ASTM N155 UNS R30155 Alloy Round Bar ASTM N155 Superalloy Round Bar UNS R30155 Bar and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.
Q: Do you accept customization?
A: Yes. If you have special requirements for products or packaging, we can make them for you.
Q: Can you accept trial orders?
A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.
Q: How do I get samples?
A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.
Packing method
Standard Seaworthy Package,etc
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.