AISI 660 Alloy Steel Plates Superalloy Turbine Blade Steel 950 MPa Tensile Strength
AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel
Description
Our company provides AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar.
All of AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.
Products Details
AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar.
| Chemical Composition (weight%): | |
| C | ≤ 0.08 |
| Si | ≤ 1.00 |
| Mn | ≤ 2.00 |
| P | ≤ 0.040 |
| S | ≤ 0.030 |
| Cr | 13.5 ~ 16.0 |
| Ni | 24.0 ~ 27.0 |
| Mo | 1.00 ~ 1.50 |
| Ti | 1.90 ~ 2.35 |
| Cu | ≤ 0.025 |
| Al | ≤ 0.035 |
| B | 0.0010 ~ 0.010 |
| Mechanical Properties Under Final Heat Treatment: | |
| Condition / Bar: Solution treated, precipitation hardened | |
| Tensile strength, σb/≥ MPa | 950 |
| Yield strength, σ0.2/≥ MPa | 650 |
| Elonghation, δ ≥(%) | 12.0 |
| Reduction of area, ф ≥ (%) | - |
| Hardness | HB | - |
Bars and, where applicable, forgings are subjected to ultrasonic examination based on the different level according to the buyers' requirements.
The alloy is usually produced by AOD / VIM VOD followed by electroslag refining (ESR) or VAR if necessary for special purpose.
FAQ
Q: How do you control the quality?
A: We have professional inspectors to analyze the chemical composition of AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar. and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.
Q: Do you accept customization?
A: Yes. If you have special requirements for products or packaging, we can make them for you.
Q: Can you accept trial orders?
A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.
Q: How do I get samples?
A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.
Submit an enquiry for the displaying steel materials you are interested in TODAY!
Sales Engineer: sales@ss-bars.com
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.