INCOLOY Alloy 825 Round Bar Superalloy 5.5mm to 800mm Solution Annealed

Price Negotiable
Price: Negotiations
MOQ: Negotiations
Delivery Time: Ex-stock for delivery: 3-7 days Production lead time: 45-55days
Brand: PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Product Description

INCOLOY alloy 825 Alloy Round Bar 825 Superalloy Round Bar 825 Round Bar 825 Bar

 

 

Description

 

 

Our company provides INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar.

All of INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.

 

  • Material:Metal,INCOLOY alloy 27-7Mo Alloy Round Bar INCOLOY alloy 27-7Mo Round Bar 27-7Mo Bar
  • Shape:Superalloy Round Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm

  • Square bar / Flat bar: 3mm to 800mm

  • Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm

  • Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)

 

 

Products Details

 

 

INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar

Chemical Composition (weight%): Mechanical Properties Under Final Heat Treatment:

C (%): ≤ 0.04
Cr (%):≤ 21.0
Ni (%):≤42.0
Mo (%): ≤3.00
Cu (%):≤2.00

Ti(%):≤1.00

Fe(%):≤30.0

Condition: Solution annealed
Tensile strength, σb/≥ MPa: 586
Yield strength, σ0.2/≥ MPa: 241
Elonghation, δ ≥(%): 30.0

 

 

 

Applications: 

 

 

INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar,Tall oil distillation columns and equipments,etc

 

INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar

 

 

FAQ 

 

 

Q: How do you control the quality?

 

A: We have professional inspectors to analyze the chemical composition of INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.

 

 

Wooden Pallet BOX,based on the customer's special requirement,Standard Seaworthy Package,etc

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Mianyang Baoheng New Material Technology Co.,Ltd
Location Building 4A, Cross-border E-commerce Industrial Park, Shiqiaopu, High-tech Zone, Mianyang City, SC, China
Contact Person Bruce Chiu

Request A Quote

Please check your email address.
Your message must be at least 20 characters.