Mianyang Baoheng New Material Technology Co.,Ltd
                                                                                                           
Verified Supplier
Years
Since
Menu

INCOLOY 903 Alloy Steel Flat Bar Superalloy 3mm to 800mm Solution Treated

Price Negotiable
Price: Negotiations
MOQ: Negotiations
Delivery Time: Ex-stock for delivery: 3-7 days Production lead time: 45-55days
Brand: PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Product Description

INCOLOY alloy 903 Alloy Steel Flat Bar 903 Superalloy Flat Bar 903 Flat Bar 903 Alloy 

 

 

Description

 

 

Our company provides INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy.All of INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.

 

  • Material:Metal,INCOLOY alloy 903 Alloy Steel Flat Bar 903 Superalloy Flat Bar 903 Flat Bar 903 Alloy
  • Shape:Superalloy Flat Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm

  • Square bar / Flat bar: 3mm to 800mm

  • Forging piece: stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.

  • Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm

  • Sheet steel via cold rolled: T0.5 - 6mm X W6 - 1000mm X L1000 - 2000mm

  • Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)

  • Length: Fixed length or random length or based on the customer's special requirement.

 

 

Products Details

 

 

INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy

Chemical Composition (weight%): Mechanical Properties Under Final Heat Treatment:

C (%): ≤ 0.020
Si (%): -
Mn (%):-
Cr (%): -
Ni (%): ≤ 38
Mo (%): -

Al(%): ≤ 0.70
Cu (%): -

Ti(%): ≤ 1.40

Fe(%): ≤ 41.0

Co (%): ≤ 15.0

Nb (%): ≤ 3.0

Condition / Bar: Solution, ageing treated
Tensile strength, σb/≥ MPa: 1174
Yield strength, σ0.2/≥ MPa: 900
Elongation, δ ≥(%): 8.0
Reduction of area, ф ≥ (%): 10.0
Hardness | HB: 311 Min

 

 

 

Applications: 

 

INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy

combustor,aerospace craft,rocket motor,nuclear reactor,petrochemical equipments,coaly transforming,etc

 

INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy

 

 

FAQ 

 

 

Q: How do you control the quality?

 

A: We have professional inspectors to analyze the chemical composition of INCOLOY alloy 903 Alloy Steel Flat Bar 903 Superalloy Flat Bar 903 Flat Bar 903 Alloy and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.

 

 

Packing method

Wooden Pallet BOX,Standard Seaworthy Package,based on the customer's special requirement,etc

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Mianyang Baoheng New Material Technology Co.,Ltd
Location Building 4A, Cross-border E-commerce Industrial Park, Shiqiaopu, High-tech Zone, Mianyang City, SC, China
Contact Person Bruce Chiu

Request A Quote

Please check your email address.
Your message must be at least 20 characters.