INCONEL alloy700 Alloy Steel Flat Bar INCONEL 700 Superalloy Flat Bar INCONEL700 Bar

 

 

Description

 

 

Our company provides INCONEL alloy700 Machined Alloy Steel Flat Bar INCONEL 700 Black Superalloy Flat Bar INCONEL700 Rrough Turned Flat Bar INCONEL700 Bright Bar.

All of INCONEL alloy700 Machined Alloy Steel Flat Bar INCONEL 700 Black Superalloy Flat Bar INCONEL700 Rrough Turned Flat Bar INCONEL700 Bright Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.

 

  • Material:Metal,INCONEL alloy700 Alloy Steel Flat Bar INCONEL 700 Superalloy Flat Bar INCONEL700 Bar 
  • Shape:Superalloy Flat Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm

  • Square bar / Flat bar: 3mm to 800mm

  • Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm

  • Sheet steel via cold rolled: T0.5 - 6mm X W6 - 1000mm X L1000 - 2000mm

  • Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)

  • Length: Fixed length or random length or based on the customer's special requirement.

 

 

Products Details

 

 

INCONEL alloy700 Machined Alloy Steel Flat Bar INCONEL 700 Black Superalloy Flat Bar INCONEL700 Rrough Turned Flat Bar INCONEL700 Bright Bar

 

Chemical Composition (weight%): Mechanical Properties Under Final Heat Treatment:

C (%): ≤ 0.15
Si (%): ≤ 0.50
Mn (%): ≤ 0.50
P (%) ≤: 0.035
S (%) ≤: 0.010
Cr (%): 13.0 ~ 17.0
Ni (%): 43.0 ~48.5
Mo (%): 3.20 ~4.50
Co (%): 26.5 ~ 30.0
W (%): -
Al (%): 2.50 ~ 4.00
Cu (%): ≤ 0.10
Ti (%): 1.80 ~2.80
Fe (%): ≤ 1.50

Tensile strength, σb/≥ MPa: 650
Yield strength, σ0.2/MPa: 315
Elongation, δ ≥(%): 30.0
Reduction of area, ф ≥ (%): -
Hardness via heat treatment /HBW: -

 

 

 

Applications: 

 

INCONEL alloy700 Machined Alloy Steel Flat Bar INCONEL 700 Black Superalloy Flat Bar INCONEL700 Rrough Turned Flat Bar INCONEL700 Bright Bar

 

such as aerospace craft, rocket motor, nuclear reactor, petrochemical equipments, coaly transforming and so on

 

INCONEL alloy700 Machined Alloy Steel Flat Bar INCONEL 700 Black Superalloy Flat Bar INCONEL700 Rrough Turned Flat Bar INCONEL700 Bright Bar

 

 

FAQ 

 

 

Q: How do you control the quality?

 

A: We have professional inspectors to analyze the chemical composition of INCONEL alloy700 Alloy Steel Flat Bar INCONEL 700 Superalloy Flat Bar INCONEL700 Bar and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.

 

 

Packing method

Wooden Pallet BOX,Standard Seaworthy Package,based on the customer's special requirement,etc

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Mianyang Baoheng New Material Technology Co.,Ltd
Location Building 4A, Cross-border E-commerce Industrial Park, Shiqiaopu, High-tech Zone, Mianyang City, SC, China
Contact Person Bruce Chiu

Request A Quote

Please check your email address.
Your message must be at least 20 characters.