INCONEL 702 Superalloy Flat Bar Shot Blasted Peeled Machined 3mm to 800mm

Price Negotiable
Price: Negotiations
MOQ: Negotiations
Delivery Time: Ex-stock for delivery: 3-7 days Production lead time: 45-55days
Brand: PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Product Description

INCONEL alloy702 Alloy Steel Flat Bar INCONEL 702 Superalloy Flat Bar INCONEL702 Bar

 

 

Description

 

 

Our company provides INCONEL alloy702 Grinding Alloy Steel Flat Bar INCONEL 702 Superalloy Annealed Flat Bar INCONEL702 Quenched and Tempered Bar.

All of INCONEL alloy702 Grinding Alloy Steel Flat Bar INCONEL 702 Superalloy Annealed Flat Bar INCONEL702 Quenched and Tempered Bar conform to Military standard, nuclear power. 100% Ultrasonic test SAE AMS 2154 /SEP 1923 /GB/T 4162 / ASTM E2375 /EN 10228-3.

 

  • Material:Metal,INCONEL alloy693 Alloy Steel Flat Bar INCONEL 693 Superalloy Flat Bar INCONEL693 Bar
  • Shape:Superalloy Flat Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm

  • Square bar / Flat bar: 3mm to 800mm

  • Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm

  • Sheet steel via cold rolled: T0.5 - 6mm X W6 - 1000mm X L1000 - 2000mm

  • Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)

  • Length: Fixed length or random length or based on the customer's special requirement.

 

 

Products Details

 

 

INCONEL alloy702 Grinding Alloy Steel Flat Bar INCONEL 702 Superalloy Annealed Flat Bar INCONEL702 Quenched and Tempered Bar

 

Chemical Composition (weight%): Mechanical Properties Under Final Heat Treatment:

C (%): ≤ 0.10
Mn (%): ≤ 1.00
Si (%): ≤ 0.70
P (%)≤: 0.020
S (%)≤: 0.010
Cr (%): 14.0 ~ 17.0
Ni (%): Remainder
Mo (%): -
Co (%): ≤ 1.00
Ti (%): 0.25 ~ 1.00
Al (%): 2.75 ~ 3.75
Cu (%): ≤ 0.50

Form: bars and forgings
Tensile strength, σb/MPa: 910
Yield strength, σ0.2/MPa: 660
Elongation, δ(%): 35.0
Reduction of area, ф(%): 60.0
Hardness + solution annealed (HB): -

 

 

 

Applications: 

 

INCONEL alloy702 Grinding Alloy Steel Flat Bar INCONEL 702 Superalloy Annealed Flat Bar INCONEL702 Quenched and Tempered Bar

 

This alloy is generally smelt in BEF or VIM + Electroslag remelting (ESR). For a purpose of superior quality, it should be smelt via technology of vacuum refining or by agreement.
It is suitable for applications such as high tensile shafts, bolts and nuts, gears, pinions spindles and so on.

 

INCONEL alloy702 Grinding Alloy Steel Flat Bar INCONEL 702 Superalloy Annealed Flat Bar INCONEL702 Quenched and Tempered Bar

 

 

FAQ 

 

 

Q: How do you control the quality?

 

A: We have professional inspectors to analyze the chemical composition of INCONEL alloy702 Alloy Steel Flat Bar INCONEL 702 Superalloy Flat Bar INCONEL702 Bar and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. 


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1T. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.

 

 

Packing method

Wooden Pallet BOX,Standard Seaworthy Package,based on the customer's special requirement,etc

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Mianyang Baoheng New Material Technology Co.,Ltd
Location Building 4A, Cross-border E-commerce Industrial Park, Shiqiaopu, High-tech Zone, Mianyang City, SC, China
Contact Person Bruce Chiu

Request A Quote

Please check your email address.
Your message must be at least 20 characters.