14-4PH Alloy Round Bar 14-4PH Superalloy
 
 
Description


14-4PH Alloy Round Bar 14-4PH Superalloy is High temperature alloys and other special alloys

All of 14-4PH Alloy Round Bar 14-4PH Superalloy conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.

  • Material:Metal, Alloy Round Bar14-4PH
  • Shape:Alloy Round Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm
  • Forging piece: stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
  • Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm
  • Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)

 
Products Details

 

14-4PH Alloy Round Bar 14-4PH Superalloy

Chemical Composition (weight%): Mechanical Properties Under Final Heat Treatment:
C(%): 0.03
Si(%): 0.75
Mn(%): 0.35
Cr(%): 14.1
Ni(%): 4.25
Mo(%): 2.38
Co(%): —
W(%): —
Al(%): —
Cu(%): 3.25
Ti(%): —
Other(%): Nb 0.25,N 0.02
TS, σb/≥MPa: 268
YS, σ0.2≥/MPa: 782
EL, δ 5≥(%): 13
Impact, AKV≥/J: 11
 

 


Applications:


14-4PH Alloy Round Bar 14-4PH Superalloy is often used in the Aerospace, cylinders, gears, hollow shafts, landing gears, marine gas turbine, etc.

 

 

 


FAQ
 

 

Q: How do you control the quality?

 

A: We have professional inspectors to analyze the chemical composition of raw materials and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.

 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Mianyang Baoheng New Material Technology Co.,Ltd
Location Building 4A, Cross-border E-commerce Industrial Park, Shiqiaopu, High-tech Zone, Mianyang City, SC, China
Contact Person Bruce Chiu

Request A Quote

Please check your email address.
Your message must be at least 20 characters.