SAE 17-22-A Alloy Round Bar 5.5mm-800mm SAE J467b-1956 R1968 BH Superalloy
SAE 17-22-A Alloy Round Bar SAE J467b-1956 R1968 BH
Description
SAE 17-22-A Alloy Round Bar is Special Purpose Alloys (Superalloys)
All of SAE 17-22-A Alloy Round Bar SAE J467b-1956(R1968) conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.
|
Products Details
SAE 17-22-A Alloy Round Bar SAE J467b-1956(R1968)
| Chemical Composition (weight%): | Mechanical Properties Under Final Heat Treatment: |
|
C(%): 0.45
Si(%): 0.65 Mn(%): 0.55 Cr(%): 12.5 Ni(%): — Mo(%): 0.55 Co(%): — W(%): — Al(%): — Cu(%): — Ti(%): — V (%):0.30 |
Tensile strength σb≥/MPa: 1250
Yield strength σs≥/MPa: 1000 Elongation δ5≥(%): 15.0 Impact, AKV≥/J: - Annealed hardness HB: 355 min. |
Applications:
SAE 17-22-A Alloy Round Bar SAE J467b-1956 (R1968) is often used in the shafts, sickles, axes, knives, wood working drills, hammers, etc.
FAQ
Q: How do you control the quality?
A: We have professional inspectors to analyze the chemical composition of raw materials and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.
Q: Do you accept customization?
A: Yes. If you have special requirements for products or packaging, we can make them for you.
Q: Can you accept trial orders?
A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.
Q: How do I get samples?
A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.