Inconel 718 725 Nickel Based Superalloy Plate Fatigue Strength 400MPa Tensile 1000MPa
Product Description:
Nickel-based superalloys are a unique type of metals that are extremely resistant to corrosion and have a high fatigue strength of ≥400MPa. Inconel 725 is a nickel-based superalloy strip that offers superior weldability and excellent corrosion resistance. It can be used in a variety of industrial applications such as SS304 316 Nickel-based superalloys industrial square tube. This type of superalloy is also highly resistant to abrasion and impact, making it an ideal choice for many applications. Furthermore, this type of superalloy can be customized to meet customer needs as it can be produced in various widths according to their specifications.
Features:
- Product Name: Nickel-based superalloy
- Surface Finish: BA/ 2B/ NO.1/ NO.3/ NO.4/ 8K/ HL/ 2D/ 1D
- Material: Round Bar Nickel Chromium Based, Nickel Based Superalloys Inconel 601 Strip
- Elongation: ≥30%
- Thickness: According To Customer Needs
- Fatigue Strength: ≥400MPa
- Creep Strength: ≥200MPa
Technical Parameters:
| Surface Finish | BA/ 2B/ NO.1/ NO.3/ NO.4/ 8K/ HL/ 2D/ 1D |
| Alloy Type | Nickel-based |
| Corrosion Resistance | Excellent |
| Hardness | ≤250HB |
| Creep Strength | ≥200MPa |
| Thickness | According To Customer Needs |
| Elongation | ≥30% |
| Tensile Strength | ≥1000MPa |
| Weldability | Good |
| Width | According To Customer Needs |
Applications:
Nickel-based superalloys, manufactured by TISCO, are known for their outstanding performance in harsh environment applications. With no exception, the brand features 201, 301L, 301, 310S, 316L, 316, 321, 436L, 304, 439, 436, 445 alloy types. All of them boast high tensile strength up to ≥1000MPa, creep strength up to ≥200MPa and elongation up to ≥30%, as well as low hardness ≤250HB.
The superior performance of these nickel-based superalloys enables them to be used in various applications, such as round bar nickel chromium based, nickel-based superalloy and nickel based superalloys plate. The products are manufactured under strict quality control and are certified by CE. The minimum order quantity accepted is 10 tons.
The price for these nickel-based superalloys is negotiable. Furthermore, the standard waterproof package ensures its safety during transportation. Customers can expect a delivery time of 3-7 days, and payments can be made via L/C, T/T, Western Union. The manufacturers can supply 5000MT/Month.
Customization:
Brand Name: TISCO
Model Number: 201, 301L, 301, 310S, 316L, 316, 321, 436L, 304, 439, 436, 445
Place of Origin: Shanxi, China
Certification: SGS, ISO, MTC
Minimum Order Quantity: 10 Tons
Price: Negotiable
Packaging Details: Standard waterproof package
Delivery Time: 3-7DAYS
Payment Terms: L/C, T/T, Western Union
Supply Ability: 5000MT/Month
Hardness: ≤250HB
Thickness: According To Customer Needs
Weldability: Good
Creep Strength: ≥200MPa
Elongation: ≥30%
Support and Services:
Nickel-based superalloy technical support and service includes:
- Product installation and maintenance advice
- Product troubleshooting and technical assistance
- Product performance optimization and enhancement
- On-site product support and training
- Product warranty extension and renewal
Packing and Shipping:
Packaging and Shipping of Nickel-based superalloy:
- Nickel-based superalloys are usually packaged in moisture-proof bags, vacuum-sealed bags, or sealed containers.
- Nickel-based superalloys must be shipped according to the regulations to ensure that they can be safely transported without any damage.
- In order to avoid damage or contamination during shipment, appropriate packaging materials such as cushioning materials, protective films and desiccants must be used.
- It is recommended to use a dedicated transport company to ensure safe and timely delivery.
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.