Hastelloy C276 Strip Product Overview
Hastelloy C276 strip is a high-performance nickel-chromium-molybdenum alloy offering exceptional corrosion resistance, oxidation resistance, and high-temperature performance. This versatile material is widely used across demanding industrial applications.
Key Product Features
- Exceptional corrosion resistance in diverse chemical environments
- High temperature strength up to 1370°C melting point
- Excellent resistance to pitting, crevice corrosion, and stress corrosion cracking
- Customizable sizes for specific application requirements
- Superior mechanical properties including 690 MPa tensile strength
Technical Specifications
| Property | Value |
|---|---|
| Material | Hastelloy C276 (UNS N10276) |
| Density | 8.22 G/cm³ |
| Melting Point | 1325-1370°C |
| Tensile Strength | 690 MPa |
| Yield Strength | 310 MPa |
| Hardness | HRB 89 |
| Young's Modulus | 220 GPa |
| Thermal Conductivity | 9.9 W/m·K |
| Coefficient of Thermal Expansion | 11.2 μm/m·K |
| Electrical Resistivity | 1.2 μΩ·m |
Available Grades & Dimensions
We offer multiple Hastelloy grades including HC-276, C-22, C-4, B2, B3, and N with customized thickness, width, and length options.
Chemical Composition Comparison
| Element | HC-276 | C-22 | C-4 | B2 | B3 | N |
|---|---|---|---|---|---|---|
| C | ≤0.01 | ≤0.015 | ≤0.015 | ≤0.02 | ≤0.01 | 0.04-0.08 |
| Mn | ≤1 | ≤0.5 | ≤1 | ≤1 | ≤3 | ≤1 |
| Fe | 4-7 | 2-6 | ≤3 | ≤2 | ≤1.5 | ≤5 |
| Cr | 14.5-16.5 | 20-22.5 | 14-18 | ≤1 | ≤1.5 | 6-8 |
| Mo | 15-17 | 12.5-14.5 | 14-17 | 26-30 | ≤28.5 | 15-18 |
Industrial Applications
- Chemical Processing: Valves, pipes, and reactors handling corrosive chemicals
- Oil & Gas: Offshore drilling equipment and production systems
- Aerospace: Gas turbine engines and aircraft exhaust components
- Nuclear Power: Critical components requiring radiation resistance
- Pollution Control: Scrubbers and flue gas desulfurization systems
Customization & Quality Assurance
Our Hastelloy strips are available in customized sizes with standard widths including 600mm, 1000mm, 1219mm, 1500mm, and lengths up to 6000mm. All products include mill test certificates and meet international standards including ASTM, DIN, and GB.
Contact Information
Email: victory@dlx-alloy.com
We welcome OEM & ODM service requests and offer competitive pricing for Hastelloy C276 strip products.
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.
Company
Changzhou Victory Technology Co., Ltd
Location
NO.32 West Taihu Road, Xinbei District, Changzhou, Jiangsu
Contact Person
Victory