Hastelloy Cobalt-Based Superalloy with 1260-1355℃ Heat Resistance and 350 MPa Yield Strength
Victory Hastelloy Alloy is a premium cobalt-based reinforced superalloy engineered for exceptional performance in extreme environments. With outstanding heat resistance up to 1355℃ and superior corrosion resistance, this nickel-molybdenum alloy delivers reliable performance in demanding industrial applications.
Operating range: 1260~1355℃ with high heat resistance
NI Rem%, CR20-22.5%, MO12.5-14.5%
Yield strength: 350 MPa
Coefficient of thermal expansion: 12.4 μm/m°C
| Parameter | Value |
|---|---|
| Available Grades | B-2, B-3, C-22, C276, C4 |
| Equal Grade Standards | UNS N10276, Hastelloy C276 |
| Alloy Type | Cobalt-based Reinforced Superalloy |
| Surface Finish | Bright, Oxided |
| Material Form | Solid (Not Powder) |
| Industry Standards | SB622 / SB619 / SB626 / SB366 / SB564 |
- Chemical processing equipment (reactors, heat exchangers)
- Pharmaceutical manufacturing systems
- Gas turbine components and furnace parts
- Marine engineering and aerospace applications
- Power generation and oil & gas industry equipment
Hastelloy C-22 grade provides exceptional resistance to both oxidizing and reducing environments, while C-276 grade offers enhanced protection against pitting, crevice corrosion, and stress corrosion cracking in chloride environments.
- Brand: Victory - Model: Hastelloy Alloy
- Place of Origin: China
- Available forms: Sheets, plates, bars, tubes, pipes
- Standard export packing with secure wooden crates
- Multiple price terms: Ex-Work, FOB, CNF, CFR, CIF, FCA, DDP, DDU
Comprehensive technical support including product selection assistance, installation guidance, maintenance protocols, and troubleshooting services. We provide training, repair, refurbishment, and custom fabrication to meet specific application requirements.
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.