Hunan Dinghan New Material Technology Co., LTD
                                                                                                           
Verified Supplier
28 Years
Since 1998
Menu

Superalloys Nickel Alloy Sheets Incoloy 825 for Petrochemical Power Generation

Price Negotiable
Price: Negotiable
MOQ: Negotiable
Delivery Time: (Sample order) 7 days
Brand: DINGSCO
Product Description

Superalloys Nickel Alloy Sheets Incoloy 825 Petrochemical Power Generation

 

Incoloy 825 and 925 nickel alloy sheets are specialized materials developed to meet the rigorous demands of the petroleum, chemical, and power generation industries, thanks to their outstanding durability, corrosion resistance, and performance at high temperatures.


Incoloy 825 Sheets:

  • Composition: Primarily composed of nickel, chromium, and molybdenum, with additional elements like copper, titanium, and iron. This unique blend provides excellent resistance to oxidation and a wide range of corrosive environments.
  • Properties: Incoloy 825 exhibits remarkable resistance to corrosion and oxidation, particularly in environments with sulfuric and phosphoric acids.It is also resistant to pitting and crevice corrosion, making it suitable for chemical processing applications.
  • Applications: Commonly used in chemical processing, pollution-control equipment, oil and gas piping, nuclear fuel reprocessing, and acid production.

 

Incoloy 825 sheets are known for their ability to maintain structural integrity under high temperature and pressure conditions, making them indispensable in applications where durability and reliability are critical. Their high-performance characteristics ensure that they are a preferred choice for challenging industrial applications where standard materials might fail.

Grade UNS Density Tensile Strength
(MPa min)
Yield Strength
(MPa min)
Reduction of Area ,min (%) Elongation min (%) Hardness (HRC)
INCOLOY 825 N08825 8.14 586MPa min 241MPa min / 30% min HRC 35max


Chemical Composition(%):
 

INCOLOY 825 Ni C Fe Mn Cr S Mo
38.0-46.0 0.05max 22.0min 1.0max 19.5-23.5 0.03max 2.5-3.5
Si Cu Al Ti      
0.5max 1.5-3.0 0.2max 0.6-1.2      

 

 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Hunan Dinghan New Material Technology Co., LTD
Location No. 2319, Building 2, Dongfang Furong Garden, No. 582 Yuanda 1st Road, Hehuayuan Street,Furong District, Changsha, Hunan Province, China.
Contact Person Julia Wang

Request A Quote

Please check your email address.
Your message must be at least 20 characters.