GH4169 alloy is a high-strength nickel-based superalloy with excellent thermal stability and oxidation resistance

Price Negotiable
Price: Price is negotiated based on the required specifications and quantity
MOQ: 100KG
Delivery Time: 5-8 working days, depending on the parameters required for negotiation
Brand: Zhonggong Special Metallurgy
Product Description

GH4169 Alloy

GH4169 is a high-performance nickel-based superalloy specifically designed for excellent strength and stability at elevated temperatures. It is widely used in demanding applications requiring exceptional thermal and oxidative resistance.

Key Features:

  • Composition: Composed primarily of nickel, with significant amounts of chromium, iron, and cobalt, along with molybdenum and titanium. This composition contributes to the alloy's outstanding mechanical properties and resistance to high-temperature degradation.
  • Temperature Resistance: GH4169 maintains its structural integrity and performance at temperatures up to approximately 1400°C (2550°F), making it suitable for extreme thermal environments.
  • Mechanical Strength: The alloy offers high yield and tensile strength, providing durability and reliability in high-stress applications.
  • Oxidation and Corrosion Resistance: GH4169 exhibits excellent resistance to oxidation and high-temperature corrosion, ensuring long-term performance and minimal degradation in harsh conditions.
  • Applications: It is commonly used in aerospace components, gas turbines, and other high-temperature industrial processes where strength, stability, and resistance to environmental factors are critical.

GH4169’s combination of high strength, thermal stability, and corrosion resistance makes it an ideal choice for applications requiring reliable performance under severe conditions.


This description emphasizes the key properties and typical uses of GH4169 alloy, highlighting its suitability for high-performance applications.

 

Here’s a detailed composition table for GH4169 alloy:

Element Content Range
Nickel (Ni) Balance
Chromium (Cr) 19.0-21.0%
Iron (Fe) 16.0-18.0%
Cobalt (Co) 8.0-10.0%
Molybdenum (Mo) 2.5-3.0%
Titanium (Ti) 1.8-2.2%
Aluminum (Al) 1.0-1.5%
Boron (B) 0.005-0.015%

This table provides a clear overview of the chemical composition of GH4169 alloy, detailing the content ranges of its key elements.

 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.
Location New South Stainless Steel Trading Market, Fangcheng Avenue, Wuxi City, Jiangsu Province, 12-101.
Contact Person Zhou

Request A Quote

Please check your email address.
Your message must be at least 20 characters.