GH738 Alloy is a nickel-based superalloy with high strength and oxidation resistance

Price Negotiable
Price: Price is negotiated based on the required specifications and quantity
MOQ: 100KG
Delivery Time: 5-8 working days, depending on the parameters required for negotiation
Brand: Zhonggong Special Metallurgy
Product Description

GH738 Alloy is a high-performance, nickel-based superalloy engineered for exceptional mechanical strength and superior oxidation resistance at elevated temperatures. It is commonly used in aerospace and industrial gas turbine applications due to its ability to maintain structural integrity under extreme conditions.

Key Features:

  • Composition: Primarily nickel, with additions of chromium, cobalt, and other elements for enhanced high-temperature stability and strength.
  • Mechanical Properties: Provides high tensile and yield strength, excellent fatigue resistance, and good ductility.
  • Thermal Stability: Retains mechanical properties over a broad temperature range, making it suitable for high-temperature environments.
  • Oxidation Resistance: Exhibits outstanding resistance to oxidation and corrosion, contributing to longer service life in harsh conditions.
  • Applications: Ideal for components such as turbine blades, vanes, and other critical parts in aerospace engines and industrial turbines.

GH738 Alloy’s robust performance characteristics make it a preferred choice for demanding applications where reliability and durability are paramount.

 

Here’s a table detailing the typical chemical composition of GH738 Alloy:

Element Content (%)
Nickel (Ni) 50.0 - 60.0
Chromium (Cr) 20.0 - 25.0
Cobalt (Co) 7.0 - 10.0
Molybdenum (Mo) 3.0 - 5.0
Titanium (Ti) 2.5 - 4.0
Aluminum (Al) 1.5 - 2.5
Iron (Fe) Balance
Carbon (C) ≤ 0.08
Boron (B) ≤ 0.01
Other Elements Traces

This composition provides GH738 Alloy with its high-temperature strength and resistance to oxidation and corrosion.

 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.
Location New South Stainless Steel Trading Market, Fangcheng Avenue, Wuxi City, Jiangsu Province, 12-101.
Contact Person Zhou

Request A Quote

Please check your email address.
Your message must be at least 20 characters.