Inconel X 750 Aerospace Springs Bolts AMS 5667 High Strength Creep Resistant Superalloy
Inconel X-750 Aerospace Springs & Bolts | AMS 5667 Certified | High-Strength, Creep-Resistant Superalloy for Extreme Environments
Inconel X750 rods are crafted from a nickel-chromium alloy renowned for its exceptional strength and corrosion resistance across a broad temperature spectrum. Enhanced with aluminum and titanium, this precipitation-hardenable alloy maintains high tensile and creep-rupture properties up to approximately 1300°F (700°C), making it ideal for demanding environments such as gas turbines, rocket engines, and nuclear reactors.
Chemical Composition
| Element | Composition (%) |
|---|---|
| Nickel (Ni) | 70 min |
| Chromium (Cr) | 14.0–17.0 |
| Iron (Fe) | 5.0–9.0 |
| Titanium (Ti) | 2.25–2.75 |
| Aluminum (Al) | 0.40–1.00 |
| Niobium (Nb) | 0.70–1.20 |
| Manganese (Mn) | ≤1.00 |
| Silicon (Si) | ≤0.50 |
| Sulfur (S) | ≤0.01 |
| Copper (Cu) | ≤0.50 |
| Carbon (C) | ≤0.08 |
| Cobalt (Co) | ≤1.00 |
Mechanical Properties
| Property | Value |
|---|---|
| Tensile Strength | 160–185 ksi |
| Yield Strength (0.2% Offset) | 100–130 ksi |
| Elongation | ≥20% |
| Hardness | 27–40 HRC |
Physical Properties
| Property | Value |
|---|---|
| Density | 0.299 lb/in³ (8.28 g/cm³) |
| Melting Range | 2540–2600°F (1393–1427°C) |
| Thermal Expansion | 7.0 x 10⁻⁶ in/in/°F (70–212°F) |
| Modulus of Elasticity | 31.0 x 10³ ksi (tension) |
Applications of Inconel X750 Rods
-
Aerospace Components: Utilized in gas turbines and rocket engines for components like turbine blades and seals due to its high-temperature strength.
-
Nuclear Reactors: Employed in reactor core components, benefiting from its corrosion resistance and mechanical stability under radiation.
-
Industrial Springs and Fasteners: Ideal for high-stress applications requiring excellent relaxation resistance at elevated temperatures.
-
Oil and Gas Equipment: Suitable for downhole and wellhead components, offering durability in corrosive environments.
Frequently Asked Questions
Q: What heat treatments are applicable to Inconel X750 rods?
A: Inconel X750 rods can undergo various heat treatments, including solution annealing and precipitation hardening, to achieve desired mechanical properties.
Q: Are Inconel X750 rods suitable for cryogenic applications?
A: Yes, they maintain excellent mechanical properties even at cryogenic temperatures, making them versatile for various temperature extremes.
Q: How does Inconel X750 compare to other nickel alloys in terms of corrosion resistance?
A: Inconel X750 offers superior corrosion and oxidation resistance, particularly in high-temperature environments, compared to many other nickel alloys.