Product Description
GH3039 Corrosion Resistant Nickel Based Superalloy
High-performance nickel-based superalloy with 8.23 g/cm³ density, designed for extreme temperature and corrosive environments.
Key Attributes
| Attribute | Value |
|---|---|
| Composition | Nickel-based superalloy containing Chromium, Cobalt, Iron, and other elements |
| Density | 8.23 g/cm³ |
| Melting Point | 1320-1370°C (2408-2498°F) |
| Tensile Strength | 850-1100 MPa (at room temperature) |
| Yield Strength (0.2% offset) | 450-700 MPa |
| Elongation | 30-50% |
| Thermal Conductivity | 9.8 W/m·K (at 100°C) |
| Coefficient of Thermal Expansion | 13.6 µm/m·K (20-100°C) |
| Electrical Resistivity | 1.10 µΩ·m (at 20°C) |
| Magnetic Properties | Non-magnetic |
Product Description
GH3039 is a premium nickel-based superalloy engineered for demanding applications requiring exceptional mechanical strength, oxidation resistance, and corrosion resistance. Its unique composition maintains structural integrity at temperatures up to 1370°C (2498°F), making it ideal for extreme environments.
Primary Applications: Gas turbine components, aerospace parts, chemical processing equipment, and other high-temperature industrial applications where reliability under prolonged stress is critical.
Detailed Composition
| Element | Composition (%) |
|---|---|
| Nickel (Ni) | 51.0 - 55.0 |
| Chromium (Cr) | 19.0 - 22.0 |
| Cobalt (Co) | 15.0 - 20.0 |
| Iron (Fe) | 5.0 - 9.0 |
| Molybdenum (Mo) | 2.5 - 3.5 |
| Titanium (Ti) | ≤ 0.70 |
| Aluminum (Al) | ≤ 0.60 |
| Carbon (C) | ≤ 0.08 |
| Manganese (Mn) | ≤ 0.50 |
| Silicon (Si) | ≤ 0.50 |
| Phosphorus (P) | ≤ 0.015 |
| Sulfur (S) | ≤ 0.010 |
| Boron (B) | ≤ 0.006 |
Performance Advantages
- Exceptional creep and fatigue resistance for prolonged service life
- Maintains mechanical properties at extreme temperatures
- Superior resistance to oxidation and corrosion
- Non-magnetic properties for specialized applications
- Reliable performance in aggressive chemical environments
Similar Products
Related Videos
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.
Company
Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.
Location
New South Stainless Steel Trading Market, Fangcheng Avenue, Wuxi City, Jiangsu Province, 12-101.
Contact Person
John zhou