User Friendly Differential Scanning Calorimeter with Touch Screen Interface
Product Overview

This touch-screen DSC instrument is specially developed for the test of oxidation induction time of polymer materials, supporting user-friendly one-key operation and fully automatic control via dedicated software.

Compliance Standards
  • GB/T 19466.2-2009 / ISO 11357-2:1999
  • GB/T 19466.3-2009 / ISO 11357-3:1999
  • GB/T 19466.6-2009 / ISO 11357-6:1999
Key Features
  • Industrial-grade wide-screen touch panel displaying comprehensive operating data
  • USB communication port with strong compatibility and automatic reconnection
  • Compact furnace chamber structure with adjustable heating and cooling rates
  • Upgraded mechanical fixing assembly prevents signal interference
  • Electric heating with compressor refrigeration cooling system
  • Dual temperature probes for high repeatability measurements
  • Automatic dual gas channel switching with fast stabilization
  • Standard sample included for convenient calibration
  • Software compatible with multiple screen resolutions and Windows operating systems
  • Customizable operating modes for full automation of testing procedures
  • Fully enclosed support structure prevents contamination
Technical Parameters
Parameter Specification
Temperature range 0℃~500℃
Temperature resolution 0.01℃
Heating rate 0.1~40℃/min
Cooling rate 0.1~20℃/min
Calorimetric resolution 100%
Constant temperature 5℃~500℃
Temperature control mode Heating, cooling, constant temperature
DSC range 0~±500mW
DSC resolution 0.01mW
Working power AC 220V 50Hz 300W or other
Atmosphere control gas Two-channel automatic control (nitrogen and oxygen)
Gas flow 0-200mL/min
Gas flow accuracy 0.2mL/min
Crucible Aluminium crucible Φ6.6*3mm (Diameter * Height)
Calibration standard With standard material (indium, tin, zinc)
Data interface Standard USB interface
Display mode 7-inch touch screen
Output mode Computer and printer
Standard Configuration
  • DSC machine: 1 set
  • Aluminium crucibles: 300 pieces
  • Power cords and USB cable: Each one
  • CD (contains software and operations video): One
  • Soft-key: One
  • Oxygen airway and nitrogen airway: Each 5m
  • Operation manual: One
  • Standard sample (contains Indium, tin, zinc): Each one
  • Tweezer and medicine spoon: Each one
  • Custom pressure reducing valve joint and quick joint: Two
  • Fused glass fuses: Four
  • External circulation thermostat sink: One
  • Water pipe: One
Product Images

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Beijing Tonghe Testing Machine Co., ltd
Location No. 1, Fengguan Road, Fengtai District, Beijing
Contact Person Zoe Bao

Request A Quote

Please check your email address.
Your message must be at least 20 characters.