Nichrome Wire NiCr 2080 Resistance Alloy Wire Cr20Ni80 Wire For Baking Equipment
- Cr20ni80 Heating Resistance Wire
In resistance heaters, Cr20Ni80 resistance wire is a commonly used heating element material. It is composed of 20% chromium and 80% nickel, with excellent electrical resistance characteristics and high temperature stability, suitable for various heating applications.
- Material Characteristics
1. Cr20Ni80 resistance wire possesses excellent oxidation resistance and high-temperature stability, making it suitable for heating elements in baking equipment.
2. Its high resistivity and low temperature drift ensure stable heating in baking equipment, allowing food to be evenly heated.
- Uniform Heating
1. Using Cr20Ni80 resistance wire as heating elements in baking equipment ensures uniform heating of food, preventing localized overheating or undercooking.
2. This uniform heating effect ensures the quality and taste of food during the baking process.
- Application Areas
1. Cr20Ni80 resistance wire is widely used in household ovens, bread makers, toaster ovens, and other baking equipment.
2. Whether in home kitchens or bakeries, Cr20Ni80 resistance wire plays a crucial role in providing stable and reliable heating solutions for various baking needs.
- Nickel-chromium alloy performance tables
| Performance material | Cr10Ni90 | Cr20Ni80 | Cr30Ni70 | Cr15Ni60 | Cr20Ni35 | Cr20Ni30 | |
| Composition | Ni | 90 | Rest | Rest | 55.0~61.0 | 34.0~37.0 | 30.0~34.0 |
| Cr | 10 | 20.0~23.0 | 28.0~31.0 | 15.0~18.0 | 18.0~21.0 | 18.0~21.0 | |
| Fe | -- | ≤1.0 | ≤1.0 | Rest | Rest | Rest | |
| Maximum temperature℃ | 1300 | 1200 | 1250 | 1150 | 1100 | 1100 | |
| Meltiing point ℃ | 1400 | 1400 | 1380 | 1390 | 1390 | 1390 | |
| Density g/cm3 | 8.7 | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 | |
| Resistivity | -- | 1.09±0.05 | 1.18±0.05 | 1.12±0.05 | 1.00±0.05 | 1.04±0.05 | |
| μΩ·m,20℃ | |||||||
| Elongation at rupture | ≥20 | ≥20 | ≥20 | ≥20 | ≥20 | ≥20 | |
| Specific heat | -- | 0.44 | 0.461 | 0.494 | 0.5 | 0.5 | |
| J/g.℃ | |||||||
| Thermal conductivity | -- | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 | |
| KJ/m.h℃ | |||||||
| Coefficient of lines expansion | -- | 18 | 17 | 17 | 19 | 19 | |
| a×10-6/ | |||||||
| (20~1000℃) | |||||||
| Micrographic structure | -- | Austenite | Austenite | Austenite | Austenite | Austenite | |
| Magnetic properties | -- | Nonmagnetic | Nonmagnetic | Nonmagnetic | Weak magnetic | Weak magnetic | |