Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy

Price Negotiable
Price: Available per request
MOQ: 50KG
Delivery Time: 30-40days
Brand: AIWEN
Product Description

Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy

Specifications of Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy:

AMS 5608, AMS 5801
EN 2.4683
PWA 1042
UNS R30188
Werkstoff 2.4683

Features of Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy:

Strength and oxidation resistant to 2000°F
Good post-aging ductility
Resistant to sulfate deposit hot corrosion

Applications of Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy:

Gas turbine engine combustor cans
Spray bars
Flame-holders and afterburner liners

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Suzhou Xunshi New Material Co., Ltd
Location No.2 Xugongqiao Road, Kunshan, 215332 China
Contact Person Allen Sun

Request A Quote

Please check your email address.
Your message must be at least 20 characters.