ISO 11357 Plastics Differential Scanning Calorimetry DSC Differential Scanning Calorimeter
Price:
Negotiable
MOQ:
1 set
Delivery Time:
7-10 days
Brand:
ZL
Product Description
ISO 11357 Plastics Differential Scanning Calorimetry DSC Differential Scanning Calorimeter
Advanced differential scanning calorimeter designed for precise thermal analysis of plastics in compliance with ISO 11357 standards.
Instrument Characteristics
- New metal furnace structure provides superior baseline performance and enhanced precision
- Indirect conduction heating ensures high uniformity, stability, and reduced pulse radiation
- Automatic bidirectional atmosphere flow with rapid switching and short stabilization time
- Includes protective gas input for enhanced sample protection
- USB communication interface with reliable, uninterrupted communication and self-recovery functionality
- Multi-stage temperature setting with fully automatic program control
- Industrial-grade 7-inch color touch screen with high clarity and intuitive operation
- Enhanced instrument sensitivity and measurement accuracy with bidirectional operating system
- Real-time spectrum acquisition and online data analysis software
Technical Specifications
| Parameter | ZL-DSC100A | ZL-DSC300 | ZL-DSC300C | ZL-DSC300L |
|---|---|---|---|---|
| Temperature Range | Room temperature~600℃ | -40~600℃ | -170~600℃ | -170~600℃ |
| Temperature Resolution | 0.01℃ | 0.001℃ | 0.001℃ | 0.001℃ |
| Temperature Fluctuation | ±0.1℃ | ±0.001℃ | ±0.01℃ | ±0.01℃ |
| Temperature Repeatability | ±0.1℃ | ±0.01℃ | ±0.01℃ | ±0.01℃ |
| Heating/Cooling Rate | 0.1~100℃/min | 0.1~100℃/min | 0.1~100℃/min | 0.1~40℃/min |
| Temperature Control Method | PID temperature control, temperature rise, constant temperature | PID temperature control, heating, constant temperature, cooling | PID temperature control, heating, constant temperature, cooling | PID temperature control, heating, constant temperature, cooling |
| DSC Range | 0~±600mW | 0~±800mW | 0~±600mW | 0~±600mW |
| DSC Accuracy | 0.01mW | 0.01mW | 0.01mW | 0.01mW |
| Working Power Supply | AC220V/50Hz or customized | |||
| Gas Flow Rate | 0~300mL/min | |||
| Gas Pressure | ≤5mPa | |||
| Display Method | 24-bit color, 7-inch LCD touch screen display | |||
| Data Interface | Standard USB interface | |||
Similar Products
Related Videos
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.
Company
Dongguan Zhongli Instrument Technology Co., Ltd.
Location
No.62, Xinhe Management of Area, Wanjiang District, Dongguan city, Guangdong province ,China
Contact Person
Fiona Zhong