DSC-100 Differential Scanning Calorimeter
The DSC-100 Differential Scanning Calorimeter is a precision instrument designed for thermal analysis of materials. This heat flow type differential scanning calorimeter offers excellent repeatability and high accuracy, making it particularly suitable for specific heat measurements.
Instrument Overview
Differential Scanning Calorimetry (DSC) is widely used as both a routine quality testing tool and research instrument. The DSC-100 measures temperature and heat flow associated with thermal transitions within materials, providing critical data for material characterization.
Key Applications
- Glass transition temperature measurement of polymer materials
- Cold crystallization and phase transition analysis
- Melting and crystallization behavior studies
- Product stability and shelf-life assessment
- Curing and crosslinking reaction monitoring
- Oxidation induction period determination
- Polymer material curing reaction temperature and thermal effect measurement
Measurement Principle
Samples and reference materials are placed in separate crucibles within the furnace and subjected to programmed heating. When sample and reference heat capacities are identical and no thermal effects occur, the temperature difference remains near zero, producing a smooth baseline curve. Thermal effects in the sample create temperature differences, with upward peaks indicating exothermic reactions and downward peaks representing endothermic processes.
Technical Specifications
| Parameter | ZL-DSC100A | ZL-DSC300 | ZL-DSC300C | ZL-DSC300L |
|---|---|---|---|---|
| Temperature Range | Room temperature~600℃ | -40~600℃ | -170~600℃ | -170~600℃ |
| Temperature Resolution | 0.01℃ | 0.001℃ | 0.001℃ | 0.001℃ |
| Temperature Fluctuation | ±0.1℃ | ±0.001℃ | ±0.01℃ | ±0.01℃ |
| Temperature Repeatability | ±0.1℃ | ±0.01℃ | ±0.01℃ | ±0.01℃ |
| Heating/Cooling Rate | 0.1~100℃/min | 0.1~100℃/min | 0.1~100℃/min | 0.1~40℃/min |
| DSC Range | 0~±600mW | 0~±800mW | 0~±600mW | 0~±600mW |
General Specifications
- DSC Accuracy: 0.01mW
- Power Supply: AC220V/50Hz or customized
- Gas Flow Rate: 0~200mL/min
- Gas Pressure: ≤0.5mPa
- Display: 24-bit color, 7-inch LCD touch screen
- Data Interface: Standard USB interface
Similar Products
Related Videos
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.
Company
Dongguan Zhongli Instrument Technology Co., Ltd.
Location
No.62, Xinhe Management of Area, Wanjiang District, Dongguan city, Guangdong province ,China
Contact Person
Fiona Zhong