AISI 682 INCOLOY 901 AMS 5660 Sheet Steel NiFeCr12Mo W-Nr 2.4975 Superalloy

 

 

Describe

 

Alloy 901 / 2.4975 is a nickel-chromium-molybdenum alloy containing titanium.

 

Size Range

 

Round bar / Wire rod (Diameter): 8.0 mm to 1000 mm

Square bar / Flat bar: 8.0 mm to 1000 mm

Forging piece: Stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.

Heavy/middle plate via hot rolled: T5 - 200 mm X W10 - 1000 mm X L1000-12000 mm

Sheet steel via cold rolled: T5 - 10 mm X W5 - 1000 mm X L1000 - 1000 mm

Steel strip via cold rolled: T0.5 - 8.0 mm X W10 - 200 mm X L (or in coil form)

Length: Fixed length or random length or based on the customer's special requirement.

 

 

Chemical Composition and standard

 

Incoloy 901/N90901/AISI 682

NiFeCr12Mo/2.4975 AMS 5660
ASTM Udimet 901 DIN EN 10095-2018 SAE AMS 5660L-2015


C(%): ≤0.10
Si(%): ≤0.40
Mn(%): ≤0.50
P(%)≤: 0.040
S(%)≤: 0.030
Cr(%): 11.0~14.0
Ni(%): 41.0~43.5

Mo(%): 5.30~6.50

Ti(%): 2.20~2.75

B(%): 0.01~0.02

Al(%): ≤0.35

Cu(%): ≤0.50

Fe(%): Remainder


 

C(%): ≤0.10
Si(%): ≤0.60
Mn(%): ≤2.0
P(%)≤: 0.02
S(%)≤: 0.01
Cr(%): 11.0~14.0
Ni(%): 40.0~45.0

Mo(%): 5.0~7.0

Ti(%): 2.35~3.1

Co(%): ≤1.0

Al(%): ≤0.35

Fe(%): Remainder

 

C(%): ≤0.10
Si(%): ≤0.60
Mn(%): ≤1.0
P(%)≤: 0.030
S(%)≤: 0.030
Cr(%): 11.0~14.0
Ni(%): 40.0~45.0

Mo(%): 5.0~7.0

Ti(%): 2.35~3.10

B(%): 0.01~0.02

Co(%): ≤1.0

Al(%): ≤0.35

Cu(%): ≤0.50

Pd(%): ≤5 ppm

Bi(%): ≤0.3 ppm

Se(%): ≤3 ppm

Fe(%): Remainder

 

 

 

Mechanical Properties

 

Tensile strength, σb/Mpa: ≥175

Yield Point, σs/Mpa: ≥ 125

Elongation, δ/%: 15

Reduction of Area,ψ/%: ≥19

 

Applications

 

  • aviation industry
  • ship industry
  • Industrial Sector Gas Turbines

 

Contact us

 

If you are interested in our products or have any questions, please contact our team of engineers at
sales@ss-bars.com
 

 
 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Mianyang Baoheng New Material Technology Co.,Ltd
Location Building 4A, Cross-border E-commerce Industrial Park, Shiqiaopu, High-tech Zone, Mianyang City, SC, China
Contact Person Bruce Chiu

Request A Quote

Please check your email address.
Your message must be at least 20 characters.