AMS 5674 Superalloy Flat Bar

Price Negotiable
Price: Negotiations
MOQ: 800kg
Delivery Time: Ex-stock for delivery: 3-7 days Production lead time: 30-60 days
Brand: PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Product Description

AMS 5674 Superalloy Flat Bar

 

 

Product Information

 

AMS 5674 is a high-temperature alloy steel with excellent corrosion resistance and high-temperature performance. It is an alloy of molybdenum, cobalt, chromium, and nickel, commonly used for manufacturing parts that work under high temperature stress, such as blades in turbine engines and blades and rotors in gas turbines. AMS 5674 alloy has good mechanical properties and high-temperature stability, and can be used at temperatures up to 980 ° C. In addition, the alloy has excellent corrosion resistance and can resist corrosion and oxidation in extreme environments.


Size Range
 
Round bar / Wire rod (Diameter):1.0 mm to 1000 mm
Square bar / Flat bar: 1.0 mm to 1000 mm
Forging piece: Stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
Heavy/middle plate via hot rolled: T5.0 - 1000 mm X W3 - 1000 mm X L100-1000 mm
Sheet steel via cold rolled: T1.0 - 10 mm X W1 - 1000 mm X L100 - 800 mm
Steel strip via cold rolled: T3.0 - 10 mm X W1.0 - 1000 mm X L (or in coil form)
Length: Fixed length or random length or based on the customer's special requirement.
 
 
Chemical Composition and standard

AMS 5674D

Mechanical Properties

SAE AMS 5674D

 

C(%): ≤0.08
Si(%): ≤1.00
Mn(%): ≤2.00
P(%): 0.035
S(%)≤: 0.03

Cr(%): 17.0~19.0
Ni(%)9.00~12.0
Mo(%): ≤0.75
Nb(%): 10xC~1.10

Ta(%): ≤0.05

Cu(%): ≤0.50

Fe: Remainder

 

Tensile strength,Rm/MPa: -
Yield strength,Rp/MPa: -

Elongation, A/%: -

Reduction of area, ψ/%: -

Hardness HRC: -

 

 

Applications
 

AMS 5674 is typically used to manufacture parts that operate under high temperature stress, such as blades in turbine engines and blades and rotors in gas turbines.


If you are interested in our products or have any questions, please contact our team of engineers at
sales@ss-bars.com

 

 
 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Mianyang Baoheng New Material Technology Co.,Ltd
Location Building 4A, Cross-border E-commerce Industrial Park, Shiqiaopu, High-tech Zone, Mianyang City, SC, China
Contact Person Bruce Chiu

Request A Quote

Please check your email address.
Your message must be at least 20 characters.