Mianyang Baoheng New Material Technology Co.,Ltd
                                                                                                           
Verified Supplier
Years
Since
Menu

7Mo Plus Alloy Round Bar 7Mo Plus Superalloy

Price Negotiable
Price: Negotiations
MOQ: Negotiations
Delivery Time: Ex-stock for delivery: 4-7 days Production lead time: 50-60days
Brand: PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Product Description

7Mo plus Alloy Round Bar 7Mo plus Superalloy
 
 
Description


All of 7Mo plus Alloy Round Bar 7Mo plus Superalloy conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.

  • Material:Metal, 7Mo plus Alloy Round Bar 7Mo plus Superalloy
  • Shape:Superalloy Round Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm

  • Square bar / Flat bar: 3mm to 800mm

  • Length: Fixed length or random length or based on the customer's special requirement.
  • Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm

  • Sheet steel via cold rolled: T0.5 - 6mm X W6 - 1000mm X L1000 - 2000mm

  • Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)

 
Products Details


 7Mo plus Alloy Round Bar 7Mo plus Superalloy

 

Chemical Composition (weight%):
C ≤0.03
Si ≤0.60
Mn 2.00
P ≤0.035
S ≤0.010
Cr 26.0~29.0
Ni 3.50~5.20
N 0.15~0.35
Mo 1.00~2.50
Mechanical Properties Under Final Heat Treatment:
TS, σb/MPa -
YS, σ0.2≥/MPa -
EL, δ 5≥(%) -
Reduction of area, ф ≥ (%) -
Hardness in condition of annealing +A ≤ -

 
 
Applications: 
 
7Mo plus Alloy Round Bar 7Mo plus Superalloy used most often in the produce the gas turbine in the field of aviation, naval vessels and industry, such as turbine blade, guide blade, turbine disc, etc.
 

 
 
FAQ 
 
 
Q: How do you control the quality?
 
A: We have professional inspectors to analyze the chemical composition of 7Mo plus Alloy Round Bar 7Mo plus Superalloy and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?
 
A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.
 

 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Mianyang Baoheng New Material Technology Co.,Ltd
Location Building 4A, Cross-border E-commerce Industrial Park, Shiqiaopu, High-tech Zone, Mianyang City, SC, China
Contact Person Bruce Chiu

Request A Quote

Please check your email address.
Your message must be at least 20 characters.