SA276 316Ti Stainless Steel Round Bar Diameter 5 - 350mm Custom Cutting any Length
SA276 316Ti Stainless Steel Round Bar Diameter 5 - 350mm Custom Cutting any Length
| Products | Stainless Steel Bar |
| Grade | 316Ti |
| Diameter | 5 - 350mm |
| Length | 6m or custom cutting any length as request |
| Finishing | Bright Bar / Black Surface |
| Heat Treatment | Solid Solution , ageing |
| Surface Process | Polishing , Peeling |
| Other Grade |
201 303 304 304L 309S 310S 316L 316Ti 317L 321 347 410 420 430 431 2205 2507 904L 254SMO 416 440A/B/C.etc |
| MOQ | 500 Kgs |
| Loading Port | Shanghai Port |
| Processing | Cutting |
| Packing | Wooden box or cutting as request |
This data sheet applies to stainless steel 316Ti / 1.4571 hot and cold rolled sheet and strip, semi-finished products, bars and rods, wire and sections as well as for seamless and welded tubes for pressure purposes.
Application
Construction encasement, doors, windows and armatures, off-shore modules, container and tubes for chemical tankers, warehouse and land transportation of chemicals, food and beverages, pharmacy, synthetic fibre, paper and textile plants and pressure vessels. Due to the Ti-alloy, resistance to intergranular corrosion is guaranteed after welding.
Chemical Compositions of 316Ti Stainless Steel
| Element | % Present (in product form) | |||
|---|---|---|---|---|
| C, H, P | L | TW | TS | |
| Carbon (C) | 0.08 | 0.08 | 0.08 | 0.08 |
| Silicon (Si) | 1.00 | 1.00 | 1.00 | 1.00 |
| Manganese (Mn) | 2.00 | 2.00 | 2.00 | 2.00 |
| Phosphorous (P) | 0.045 | 0.045 | 0.0453) | 0.040 |
| Sulfur (S) | 0.0151) | 0.0301) | 0.0153) | 0.0151) |
| Chromium (Cr) | 16.50 - 18.50 | 16.50 - 18.50 | 16.50 - 18.50 | 16.50 - 18.50 |
| Nickel (Ni) | 10.50 - 13.50 | 10.50 - 13.502) | 10.50 - 13.50 | 10.50 - 13.502) |
| Molybdenum (Mo) | 2.00 - 2.50 | 2.00 - 2.50 | 2.00 - 2.50 | 2.00 - 2.50 |
| Titanium (Ti) | 5xC to 070 | 5xC to 070 | 5xC to 070 | 5xC to 070 |
| Iron (Fe) | Balance | Balance | Balance | Balance |
Mechanical properties of 316Ti Stainless Steel
| Product Form | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| C | H | P | L | L | TW | TS | |||
| Thickness (mm) Max | 8 | 12 | 75 | 160 | 2502) | 60 | 60 | ||
| Yield Strength | Rp0.2 N/mm2 | 2403) | 2203) | 2203) | 2004) | 2005) | 1906) | 1906) | |
| Rp1.0 N/mm2 | 2703) | 2603) | 2603) | 2354) | 2355) | 2256) | 2256) | ||
| Tensile Strength | Rm N/mm2 | 540 - 6903) | 540 - 6903) | 520 - 6703) | 500 - 7004) | 500 - 7005) | 490 - 6906) | 490 - 6906) | |
| Elongation min. in % | A1) %min (longitudinal) | - | - | - | 40 | - | 35 | 35 | |
| A1) %min (transverse) | 40 | 40 | 40 | - | 30 | 30 | 30 | ||
| Impact Energy (ISO-V) ≥ 10mm thick | Jmin (longitudinal) | - | 90 | 90 | 100 | - | 100 | 100 | |
| Jmin (transverse) | - | 60 | 60 | 0 | 60 | 60 | 60 | ||
Reference data on some physical properties
| Density at 20°C kg/m3 | 8.0 | |
|---|---|---|
| Modulus of Elasticity kN/mm2 at | 20°C | 200 |
| 200°C | 186 | |
| 400°C | 172 | |
| 500°C | 165 | |
| Thermal Conductivity W/m K at 20°C | 15 | |
| Specific Thermal Capacity at 20°C J/kg K | 500 | |
| Electrical Resistivity at 20°C Ω mm2 /m | 0.75 | |
Processing / Welding
Standard welding processes for this steel grade are:
- TIG-Welding
- MAG-Welding Solid Wire
- Arc Welding (E)
- Laser Beam Welding
- Submerged Arc Welding (SAW)




Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.