Hot Rolled S31803 Duplex Steel Plate 2205 Stainless Steel Plate with Chloride Stress Corrosion Resistance and High Strength

Price Negotiable
Price: US $3.35 / kg
MOQ: 20 kg
Delivery Time: Negotiable
Product Description
S31803 Duplex Steel Plate S32205 2205 Stainless Steel Plate
2205 is a duplex (austenitic-ferritic) stainless steel containing about 40-50% ferrite in the annealed condition. This alloy provides a practical solution to chloride stress corrosion cracking problems experienced with 304/304L or 316/316L stainless steels. The high chromium, molybdenum, and nitrogen contents provide corrosion resistance superior to 316/316L and 317L stainless in most environments. Note that 2205 is not recommended for operating temperatures above 600°F.
The design strength of 2205 is significantly higher than 316/316L, often permitting lighter wall construction. This alloy maintains good notch impact toughness down to temperatures below -40°F and is welded with E2209 or ER2209 fillers.
Key Features
  • High resistance to chloride stress corrosion cracking
  • Chloride pitting and crevice corrosion resistance superior to 317L stainless
  • Good general corrosion resistance
  • High strength
  • Good sulfide stress corrosion resistance
  • Useful up to 600°F
Applications
  • Chemical process vessels, piping, and heat exchangers
  • FGD scrubber systems
  • Pulp mill digesters, bleach washers, chip presteaming vessels
  • Food process equipment
  • Oil field piping, heat exchangers
Specifications
UNS S31803
ASME SA-182 (F51), SA-240, SA-798, SA-790, SA-815
ASTM A182 (F51), A240, A276, A479, A789, A790, A815, A928, A988
SAE J405
UNS S32205
ASME SA-182 (F60), SA-240, SA-798, SA-790, SA-815
ASTM A182 (F60), A240, A276, A479, A480, A798, A790, A815, A928, A988
SAE J405
S31803/S32205 Duplex Steel Plate close-up showing material texture and surface finish
2205 Stainless Steel Plate industrial application in manufacturing environment

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company JIANGSU MITTEL STEEL INDUSTRIAL LIMITED
Location No.283-1, Youyi Middle Road, Xishan District, Wuxi City, Jiangsu Province
Contact Person Gao Ben

Request A Quote

Please check your email address.
Your message must be at least 20 characters.