4J42 Corrosion Resistant Alloy Rod For Aerospace Composites

Price Negotiable
Price: To negotiate
MOQ: 200KG
Delivery Time: 45~60days
Brand: KAIXIN
Product Description

KX 4J42 Corrosion Resistant Alloy Light Rod On Expansion Alloy

 

Product Description and Application

 

4J42 Fe-Ni constant expansion alloy is a series of constant expansion alloys which can be matched with soft glass and ceramic with different expansion coefficient in a given temperature range by adjusting the nickel content. The expansion coefficient and Curie point of 4J42 Fe-Ni constant expansion alloy would increase with the nickel content increase . The alloy is a widely used sealing structure material in the electric vacuum industry, which is used to match the sealing with soft glass and ceramic on the production of electrical components, matching and sealing with corresponding soft glass in electric vacuum industry.
 

Process Performance and Requirements
 

  • Product Fusion Process

 
Vacuum Induction Furnace(VIM) and Electroslag Remelting Furnace(ESR)
 

  • Product Chemical Composition 

 

Alloy Grade C P S Mn Si Al Co Ni Fe
4J42 ≤0.05 ≤0.02 ≤0.02 ≤0.8 ≤0.3 ≤0.1 ≤1 41.0~42.5 Rem

 
 

  • Product Physical Property

 

Density 8.1g/cm3
Melting Point 1430℃

 

  • Product Wire Tensile Strength

 

State Code State Tensile strength/MPa
R Soft <590
I Hard >820

 

  • Product Strip Physical Property

 

State Code State Tensile Strength/MPa
R Soft <570
I Hard >700

 

  • Product Average Linear Expansion Coefficient

 

Alloy Grade Sample Heat Treatment Institution

Average Coefficient of Linear Expansion

α(10-6/ K)

20~ 300 oC 20~ 400 oC 20~ 450 oC
4J42 It is heated to 900±20 oC in hydrogen atmosphere, insulated lh, and cooled to less than 200 oC at a speed of no more than 5 oC/ min 4.0~ 5.0 ------ 6.5~7.5

 

  • Product Typical Average Linear Expansion Coefficient

 

Alloy Grade

Average Coefficient of Linear Expansion  α(10-6/ K)

20~100℃ 20~200℃ 20~300℃ 20~400℃ 20~450℃ 20~500℃ 20~600℃
4J42 5.6 4.9 4.8 5.9 6.9 7.8 9.2

 

  • Productive Process

 

 

  • Professional Customization

Cold-drawn Wire ¢0.3~¢18mm(Delivery in rolls or trays)
Hot-Rolling Wire ¢5.5~¢20mm(Delivery in rolls)
Strip thickness 0.1~4.5*width 6~350mm(Supply in rolls or straight strips)
Smooth Forged Rod on a Lathe

¢60~350mm,L800-2500mm

Hot-rolled Burnishing ¢20~80mm,L1000-5000mm
Cold Drawn and Burnishing ¢2.5~18mm,L1000-8000mm
Seamless Tube ¢1~275mm,wall thickness 0.2~30,L1000-8000mm

 
 

 





 
 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Danyang Kaixin Alloy Material Co., Ltd.
Location The North East of Danlv Bridge, Aerospace Industry Park, Lvcheng Town,Danyang City,Jiangsu Province
Contact Person AnnaPei

Request A Quote

Please check your email address.
Your message must be at least 20 characters.