UNS N06601 W.Nr. 2.4851 Nickel Superalloy Inconel 601 Wire 1415°C High Temperature Resistance
UNS N06601/W.Nr. 2.4851 Nickel Superalloy Inconel 601 Wire 1415°C High Temperature Resistance
Product Introduction
Inconel 601 wire has a wide range of applications in the power field, mainly due to its excellent high temperature oxidation resistance, good mechanical strength and excellent corrosion resistance. This nickel chromium iron alloy has excellent performance in high temperature environment, and can resist oxidation, carbonization, vulcanization and other forms of corrosion. It is suitable for the range from low temperature to high temperature above 1250 ° C. In the power industry, Inconel 601 wire is often used to manufacture boiler components, superheater tubes, steam reforming tubes and other key components. In addition, it is also used in radiant tubes, flame hoods, annealing furnace tubes, braided conveyor belts, chain curtains, burner nozzles and electric heating elements in industrial furnaces. These applications not only require the material to remain stable at high temperature, but also need to have good processing and welding properties, and Inconel 601 wire just meets these requirements. Therefore, Inconel 601 wire is an indispensable high-performance material in the power field, which is widely used in various key equipment and structures.
Parameter
Chemical Properties of Inconel 601
| Item | C | Mn | Fe | P | S | Si | Cu | Ni | Co | Al | Ti | Cr | Nb+Ta | Mo | B |
|
Inconel 601
|
≤0.1 | ≤1.5 | rest | ≤0.02 | ≤0.015 | ≤0.5 | ≤1 | 58-63 | -- | 1-1.7 | -- | 21-25 | -- | -- | -- |
| ITEM | θ/℃ | TENSIE STRENGTH | HBS | |||
| σb/MPa | σP0.2/MPa | δ5/% | φ/% | |||
| BAR/ROD | 20 | ≥585 | ≥240 | ≥30 | - | 134~217 |
| RING | 20 | ≥520 | ≥205 | ≥35 | - | ≥187 |
| HOT ROLL PLATE | 20 | ≥550 | ≥240 | ≥35 | ≥40 | - |
| 900 | ≥95 | ≥45 | ≥40 | ≥50 | - | |
| COLD ROLLED SHEET | 20 | ≥550 | ≥240 | ≥30 | - | - |
| 900 | ≥90 | ≥40 | ≥60 | - | - | |
| COLD ROLLED SHEET | 20 | ≥550 | ≥200 | ≥30 | - | - |
| STRIP | 20 | ≥550 | ≥240 | ≥30 | - | - |
| WIRE | 20 | - | HV≤151 | |||
| AMS Number | Alloy | Type | UNS | Cross Ref. Spec | Misc./Shape |
|---|---|---|---|---|---|
| AMS 5715 | Inconel 601 | Nickel | N06601 | ||
| AMS 5715 Bar | Inconel 601 | Nickel | N06601 | - | Bar |
| AMS 5715 Custom Tube | Inconel 601 | Nickel | N06601 | - | Custom Tube |
| AMS 5715 Forging | Inconel 601 | Nickel | N06601 | - | Forging |
| AMS 5715 Ring | Inconel 601 | Nickel | N06601 | - | Ring |
| AMS 5870 | Inconel 601 | Nickel | N06601 | ||
| AMS 5870 Plate | Inconel 601 | Nickel | N06601 | - | Plate |
| AMS 5870 Sheet | Inconel 601 | Nickel | N06601 | - | Sheet |
| AMS 5870 Strip | Inconel 601 | Nickel | N06601 | - | Strip |
Specific Applications
In the power sector, Inconel 601 wire is widely used in the following equipment and components:
- Superheater pipe support: used to support the superheater pipe to ensure stability and safety in high temperature and high pressure environment.
- Grid barrier: used to protect equipment from high temperature and corrosive gases.
- Ash treatment system: used to treat high-temperature ash to ensure long-term stable operation of the system.
- Burner nozzle: used for fuel injection to ensure combustion efficiency and stability.
- Resistance heating element: used to manufacture resistance heating elements to ensure efficient operation in high temperature environment.
Advantages and Characteristics
- Excellent high temperature corrosion resistance:Inconel 601 has excellent oxidation resistance and carbonation resistance in high temperature environment. It can be used for a long time at temperatures up to 1180 ° C. even in the process of severe heating and cooling cycles, it can form a dense oxide film with high spalling resistance.
- Good mechanical properties:Inconel 601 has good mechanical properties at room temperature and high temperature. After annealing, the tensile strength can reach 650 n/mm ², the yield strength can reach 300 n/mm ², and the elongation can reach 30%.
- Excellent fatigue resistance:Inconel 601 has excellent fatigue resistance and can be used for a long time under a wide range of cyclic loads.
- Low permeability:Inconel 601 is usually a non-magnetic material and remains non-magnetic even at low temperatures, which makes it a unique advantage in applications that need to avoid magnetic field interference.
Contact Us
Email:fbwlau@cnrunlai.com
Oem service:
Welcome customized size
We are experience factory for OEM&ODM service
Related Questions and Answers
1. what are the advantages of Inconel 601 wire?
Inconel 601 has excellent oxidation resistance and high temperature corrosion resistance, and its mechanical properties under high temperature conditions are better than Inconel 600.
2. what are the characteristics of Inconel 601 wire?
Inconel 601 has good high temperature corrosion resistance and oxidation resistance, excellent cold and hot processing and welding properties, and satisfactory thermal strength and high plasticity below 700 ℃.
3. what are the application areas of Inconel 601 wire?
Inconel 601 is widely used in pallets, baskets and fixtures in heat treatment plants, steel wire split annealing and radiation tubes, high-speed gas burners, wire mesh belts in industrial furnaces, isolation tanks in ammonia reforming and catalytic support grids in nitric acid manufacturing, exhaust system components, combustion chambers of solid waste incinerators, etc.
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.