Silicon Steel Coil Amorphous Magnetic Core with High Saturation Magnetic Induction Low Magnetic Loss and Good Frequency Performance

Price Negotiable
Price: Negotiable
MOQ: Negotiable
Delivery Time: 10-15 work days
Product Description
Silicon Steel Coil
Product Performance
  • High saturation magnetic induction Bs
  • Low magnetic loss compared to other materials
  • Excellent frequency and temperature performance, suitable for 3000KHz applications
  • High DC bias characteristics
  • Low magnetic leakage rate
  • Lighter weight and smaller size compared to alternative materials
Technical Specifications
Density 7.3 g/cm³
Curie temperature Tc = 410°C
Essence temperature Tx = 530°C
Saturation Bs = 1.56T
Resistivity ρ = 130 Ω-cm
Saturated magnetic stretching performance λs = 27*10⁻⁶
Product Description
We provide amorphous magnetic cores for automotive audio systems and perform wire winding processing. Standard magnetic core specifications are available.
Customization Options
Magnetic cores can be customized according to customer specification drawings. Required parameters for customization include:
  • Core size and shell dimensions
  • Parameter performance AL @ DC bias = 0A and other AL values under different DC currents
  • Copper wire diameter specifications
Primary Applications
  • SMS output choke
  • DC/DC conversion choke coil
  • Ordinary mode choke
  • Choke for adapters and battery chargers
  • PFC choke
  • Car audio systems

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Foshan Mellow Stainless Steel Co., Ltd.
Location Xinbao Plaza, Tiancheng Rd, Shunde District, Foshan, Guangdong Province, China, 528041
Contact Person Ouyang

Request A Quote

Please check your email address.
Your message must be at least 20 characters.