Product Overview
The ZEMS1040 is an integrated molding power inductor designed for high-density applications. It features low DCR, ultra-high current capability, and magnetic shielding for strong anti-electromagnetic interference. Its composite construction ensures ultra-low buzz noise and high reliability with excellent vibration resistance. Suitable for various electronic devices, including PDAs, notebooks, servers, and DC/DC converters in distributed power systems.
Product Attributes
- Brand: (ZEMS)
- Origin: Dongguan, China
- Material: Low loss alloy powder
- Certifications: RoHS, Halogen Free, REACH Compliant
Technical Specifications
| Part No. | Inductance (H) | Tolerance | Test Frequency/Voltage | DCR (m) Typical | Saturation Current (A) Typical | Temperature Rise Current (A) Typical | Dimensions (LWH) (mm) |
| ZEMS1040-R015M | 0.15 | 20% | 100kHz/1.0V | 0.65 | 45.00 | 0.6 | 11.5x10x3.8 |
| ZEMS1040-R022M | 0.22 | 20% | 100kHz/1.0V | 1.40 | 35.00 | 0.7 | 11.5x10x3.8 |
| ZEMS1040-R030M | 0.30 | 20% | 100kHz/1.0V | 1.30 | 35.00 | 0.7 | 11.5x10x3.8 |
| ZEMS1040-R036M | 0.36 | 20% | 100kHz/1.0V | 1.90 | 30.00 | 0.8 | 11.5x10x3.8 |
| ZEMS1040-R047M | 0.47 | 20% | 100kHz/1.0V | 2.20 | 30.00 | 0.9 | 11.5x10x3.8 |
| ZEMS1040-R056M | 0.56 | 20% | 100kHz/1.0V | 2.40 | 25.00 | 1.0 | 11.5x10x3.8 |
| ZEMS1040-R068M | 0.68 | 20% | 100kHz/1.0V | 2.50 | 23.00 | 1.1 | 11.5x10x3.8 |
| ZEMS1040-R080M | 0.80 | 20% | 100kHz/1.0V | 2.70 | 23.00 | 1.2 | 11.5x10x3.8 |
| ZEMS1040-1R0M | 1.00 | 20% | 100kHz/1.0V | 3.30 | 19.00 | 1.5 | 11.5x10x3.8 |
| ZEMS1040-1R5M | 1.50 | 20% | 100kHz/1.0V | 4.20 | 16.00 | 2.2 | 11.5x10x3.8 |
| ZEMS1040-2R2M | 2.20 | 20% | 100kHz/1.0V | 7.50 | 12.00 | 3.3 | 11.5x10x3.8 |
| ZEMS1040-3R3M | 3.30 | 20% | 100kHz/1.0V | 11.80 | 11.00 | 4.7 | 11.5x10x3.8 |
| ZEMS1040-4R7M | 4.70 | 20% | 100kHz/1.0V | 20.00 | 9.00 | 5.6 | 11.5x10x3.8 |
| ZEMS1040-5R6M | 5.60 | 20% | 100kHz/1.0V | 22.00 | 8.50 | 6.8 | 11.5x10x3.8 |
| ZEMS1040-6R8M | 6.80 | 20% | 100kHz/1.0V | 25.00 | 8.50 | 8.2 | 11.5x10x3.8 |
| ZEMS1040-8R2M | 8.20 | 20% | 100kHz/1.0V | 27.00 | 8.00 | 10.0 | 11.5x10x3.8 |
| ZEMS1040-100M | 10.00 | 20% | 100kHz/1.0V | 37.00 | 7.80 | 15.0 | 11.5x10x3.8 |
| ZEMS1040-150M | 15.00 | 20% | 100kHz/1.0V | 55.00 | 6.50 | 22.0 | 11.5x10x3.8 |
| ZEMS1040-220M | 22.00 | 20% | 100kHz/1.0V | 66.00 | 5.00 | 33.0 | 11.5x10x3.8 |
| ZEMS1040-330M | 33.00 | 20% | 100kHz/1.0V | 92.00 | 4.40 | 47.0 | 11.5x10x3.8 |
| ZEMS1040-470M | 47.00 | 20% | 100kHz/1.0V | 155.00 | 3.30 | 56.0 | 11.5x10x3.8 |
| ZEMS1040-560M | 56.00 | 20% | 100kHz/1.0V | 155.00 | 2.80 | 68.0 | 11.5x10x3.8 |
| ZEMS1040-680M | 68.00 | 20% | 100kHz/1.0V | 220.00 | 2.50 | 82.0 | 11.5x10x3.8 |
| ZEMS1040-820M | 82.00 | 20% | 100kHz/1.0V | 185.00 | 2.30 | 100.0 | 11.5x10x3.8 |
| ZEMS1040-101M | 100.00 | 20% | 100kHz/1.0V | 290.00 | 2.00 | 100.0 | 11.5x10x3.8 |
Environmental Data
Operating Temperature: -55 to +125 (Including coils self-temperature rise)
Reliability Data
| Item | Requirements | Test Methods and Remarks |
| Operating Temperature Range | -55+125 (Including self-heating temperature rise) | |
| Solderability | 90% or more of electrode area shall be coated by new solder. | Dip pads in flux and dip in solder pot (96.5Sn/3.0Ag/0.5Cu) at 245 5 for (51) seconds. |
| Resistance to Soldering Heat | No visible mechanical damage. Inductance change: Within 10% | Dip pads in flux and dip in solder pot (96.5Sn/3.0Ag/0.5Cu) at 2605 for (101) seconds. |
| Low temperature storage | No visible mechanical damage. Inductance change: Within 10% | Store temperature -552 for total 1000hr. |
| High temperature storage | No visible mechanical damage. Inductance change: Within 10% | Store temperature 1252 for total 1000hr. |
| Static Humidity | No visible mechanical damage. Inductance change: Within 10% | Inductors shall be subjected to (933)%RH. at 40 2 for 96 h2 h. Inductors are to be tested after having air dried for 2 hours. |
| Thermal shock | No visible mechanical damage. Inductance change: Within 10% | (-403), time (303) min (852) /(303) min, conversion time (2~3) min, cycle 5 times. |
| Mechanical Shock | No evidence of terminal peel off and wire broken. | Inductors shall be Soldered on the PCB with 1.0mm thick and fixed them in a 15cm big.,1.4Kg weight cube with brass base, let it nature fallen form 0.5m height (X,Y,Z three axes). |
| Adhesion of terminal electrode | Strong bond between the pad and the core, without come off. | Inductors shall be Subjected to 260 5 for 20 s5 s Soldering in the base with 0.3mm solder. And then aplomb electrode way plus tax 10 N for 10 1s seconds. |
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.
Company
Beijing Silk Road Enterprise Management Services Co., Ltd.
Location
16 Floor, Unit B, Jiatai International Mansion, No 41, Dongsihuan Zhong Road, Chaoyang District, Beijing
Contact Person
Sellina