UNS N06600 Nickel Alloy Tube With Chloride Stress Corrosion Cracking Resistance

Price Negotiable
Price: Negotiable (Request a Quote)
MOQ: 100kg
Delivery Time: 15-25days
Brand: Baosteel,TISCO
Product Description
UNS N06600 High Temperature Nickel Alloy Tube - Heat Resistant Nickel Chromium Alloy
UNS N06600 (Inconel 600) is a nickel-chromium alloy specifically designed for high-temperature and corrosion-resistant applications. With a nominal composition of 72% Ni + 14-17% Cr, this alloy offers excellent oxidation resistance up to 1093°C (2000°F), good strength at elevated temperatures, and outstanding resistance to chloride-ion stress-corrosion cracking.
The high-temperature nickel alloy tube is widely used in heat treatment furnaces, chemical processing, aerospace components, and nuclear engineering. Its heat-resistant nickel chromium alloy composition ensures reliable performance in harsh environments where standard stainless steels would fail.
Specifications & Dimensions
Parameter Details
Standard ASTM B163, ASTM B167, ASME SB163, ASME SB167
Grade Inconel 600 / UNS N06600
Type Seamless tube / Welded tube (as required)
Outer Diameter 6.0 mm – 219.1 mm (1/8″ – 8″)
Wall Thickness 0.5 mm – 12.7 mm (SCH 5S – SCH 80S)
Length 6 m / 9 m / 12 m, or random lengths
Process Cold drawn / Cold rolled (seamless)
Finish Annealed & pickled, bright annealed
Packaging Hexagonal bundles + plastic end caps + seaworthy wooden crates or pallets
Ends Plain end / Beveled end
Chemical Composition
The unique properties of Inconel 600 derive from its high nickel content (72% minimum) combined with chromium. This balance provides resistance to both reducing (nickel) and oxidizing (chromium) environments.
Element Content (%) Role
Nickel (Ni) 72.0 min Base element – provides resistance to reducing conditions, alkaline solutions, and chloride-ion SCC
Chromium (Cr) 14.0 – 17.0 Provides resistance to oxidizing conditions, sulfur compounds, and high-temperature oxidation
Iron (Fe) 6.0 – 10.0 Adds structural stability and cost-effectiveness
Carbon (C) 0.15 max Controlled for carbide formation at elevated temperatures
Manganese (Mn) 1.0 max Deoxidizer and grain refiner
Silicon (Si) 0.50 max Enhances oxidation resistance
Copper (Cu) 0.50 max Trace element – controlled for corrosion resistance
Sulfur (S) 0.015 max Controlled for hot workability
For nuclear applications (Alloy 600T), tighter controls on cobalt, boron, and other trace elements are applied – contact us for nuclear-grade certification.
Typical Mechanical Properties (Annealed Condition)
Inconel 600 is supplied in the annealed condition (solution treated) for optimal corrosion resistance and fabricability. Cold-worked tempers (¼ hard, ½ hard, full hard) are available for wire and strip applications requiring higher strength.
Product Form Condition Tensile Strength (KSI / MPa) Yield Strength 0.2% Offset (KSI / MPa) Elongation (%) Hardness
Rod & Bar Annealed 80 – 100 (550 – 690) 25 – 50 (170 – 345) 55 – 35 65 – 85 HRB
Plate (Hot Rolled) Annealed 80 – 100 (550 – 725) 30 – 50 (205 – 345) 55 – 35 65 – 85 HRB
Sheet (Cold Rolled) Annealed 80 – 100 (550 – 690) 30 – 45 (205 – 310) 55 – 35 88 HRB max
Tube & Pipe Cold Drawn / Annealed 80 – 100 (550 – 690) 25 – 50 (170 – 345) 55 – 35 88 HRB max
Wire (Soft) Annealed 80 – 120 (550 – 830) 35 – 75 (240 – 520) 45 – 20
Wire (¼ to ½ Hard) Cold Drawn (No. 1 Temper) 105 – 135 (725 – 930) 70 – 105 (480 – 725) 35 – 15
Wire (Spring Temper) Full Hard 170 – 220 (1170 – 1520) 150 – 210 (1035 – 1450) 5 – 2
Key Features
Excellent oxidation resistance up to 1093°C (2000°F)
Good high-temperature strength and creep resistance
Outstanding resistance to chloride stress-corrosion cracking
Resistant to many organic and inorganic corrodents
Good mechanical properties at sub-zero temperatures
Easy to weld and fabricate
Applications
UNS N06600 high temperature nickel alloy tube is used in demanding environments, including:
Industry Application
Heat Treatment Furnace components, retorts, muffles, radiant tubes
Chemical Processing Reactors, heat exchangers, evaporator tubes
Aerospace Engine components, exhaust systems
Nuclear Reactor core components
Petrochemical Cracker tubes, transfer piping
Electronics Cathode ray tube support grids
Looking for a reliable supplier of UNS N06600 high-temperature nickel alloy tubes?

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Shanxi Zhongcheng Metal Co., Ltd.
Location Room 2, No. 221 Tianzhang Avenue, Fengdong New City, Xi'an, Shaanxi Province
Contact Person Zhongcheng Metal

Request A Quote

Please check your email address.
Your message must be at least 20 characters.