100um Thick Ultra Thin LiTaO3 Wafer Z Cut For Pyroelectric Applications
100um Thick Ultra-Thin LiTaO3 Z-Cut For Pyroelectric Applications
For many years the pyroelectric material lithium tantalate (LiTaO3 ) has proved itself at use in pyroelectric detectors. It fulfils not only the demands on material characteristic quantities just mentioned but also stands out due to an excellent temperature stability and very good reproducibility of the detector performance.
Typical material properties of LiTaO3 at room temperature are:
p = 1,8 . 10-8 Ccm-2K-1
εr = 43
tanδ = 0,001
cP´ = 3,2 Jcm-3K-1
|
Transparency Range |
High transmittance from 0.4 to 4um |
|
Crystal Symmetry |
Trigonal, space group C3v OR 3m |
|
Density |
7.45 |
|
Curie Temperature |
605±2℃ |
|
Mohs Hardness |
5.5 |
|
Thermal Expansion Coefficient |
αa=16.1×10^-6/k, αc=4.1×10^-6/k |
|
Refractive Indices, Birefringence |
n0=2.176, ne=2.18, Δn=0.004 at 0.63um |
|
Dielectric Constants (Relative) |
ετ11=53.6; ετ33=43.4 |
|
Pyroelectric Coeff. @27℃ |
0.019 u Coulomb/cm2/℃ |
|
Electro-Optic Coeff. @0.63um |
Γ13=7×10^-12m/v |
|
Nonlinear Optical Coeff. @1.06um |
d22=2.08×10^-12m/v |
Acceptance Check
- The product is fragile. We have adequately packed it and labeled it fragile. We deliver through excellent domestic and international express companies to ensure transportation quality.
- After receiving the goods, please handle with care and check whether the outer carton is in good condition. Carefully open the outer carton and check whether the packing boxes are in alignment. Take a picture before you take them out.
- Please open the vacuum package in a clean room when the products are to be applied.
- If the products are found damaged during courier, please take a picture or record a video immediately. DO NOT take the damaged products out of the packaging box! Contact us immediately and we will solve the problem well.
Get in Touch
Have questions about our products or want to discuss a custom order? Our team is ready to help you.