High Temperature Creep Testing Machine Compressive Creep Rate Analyzer

Price Negotiable
Price: Negotaible
MOQ: 1
Delivery Time: 5-8 work days
Brand: Lonroy
Product Description

LRHY High Temperature Creep Testing Instrument Elevated Temperature Compressive Creep Rate Analyzer

1.Description:

This instrument is used to test the resistance of refractory materials to the high-temperature load softening effect, and it is an important indicator for testing the high-temperature mechanical properties of refractory materials. It complies with the national standards GB/T5073-2005 "Test Method for Creep of Refractory Materials under Pressure" and GB/T5989-2008 "Test Method for Softening Temperature of Refractory Materials under Load", and it can conduct automatic computer testing, data processing, and automatically generate temperature and deformation curve graphs for saving.

2.Technical Parameter

Parameter Item Specification
Max. Heating Temperature 1650°C
Temperature Control ±1°C accuracy, microprocessor-programmable
Deformation Measurement Error ≤0.01mm
Sample Size Ø50 × 50 mm
Sample Load Pressure 0.2MPa
Power Supply 380V AC, 3kW
 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company DONGGUAN LONROY EQUIPMENT CO LTD
Location A31, 11 Floor, No 1 Building, Minjian Jinrong Building, No 111 Guantai Road, Sanyuanli Community, Nancheng Street, Dongguan, Guangdong, China
Contact Person Kaitlyn Wang

Request A Quote

Please check your email address.
Your message must be at least 20 characters.