Polymer Modified Asphalt Waterproof Coating For Tunnel Engineering

Price Negotiable
Price: USD 0.8‑1.0/kg
MOQ: 1000kg
Delivery Time: Negotiable
Brand: shhous
Product Description

Polymer Modified Asphalt Waterproof Coating For Tunnel Engineering

High‑Polymer Modified Asphalt Waterproof Coating Application Methods 

  1. Base Surface Treatment The base surface shall be solid, flat, clean, free of sanding, dust and oil stains. Cracks and pits shall be repaired and leveled with polymer mortar. Internal and external corners shall be formed into R50mm circular arcs. Pipe roots and water outlet peripheries shall be compactly repaired without sharp edges and corners. No standing water on the base surface, with moisture content ≤9%. A primer is recommended for loose and sanding base surfaces for reinforcement.
  2. Detailed Additional Layer (Key Point) Apply additional layers at internal and external corners, pipe roots, floor drains, expansion joints and water outlets with a width ≥200 mm, adopting the method of two‑coat‑one‑fabric: first apply a thin coat of coating, lay non‑woven fabric / polyester fabric, ensure the reinforcement fabric is fully saturated without wrinkles or edge curling. Apply another coat to cover the fabric after surface‑dry.
  3. Large‑Area Coating Construction Stir thoroughly with electric mixer after opening the drum. Do not dilute with water or solvent. Apply by roller, brush or spray. Apply multiple thin coats in cross directions; the subsequent coat shall be applied perpendicular to the previous one. Wait until the previous coat is surface‑dry and non‑tacky before applying the next coat. Interval: 2‑6 h at normal temperature; extend to 8‑24 h under low‑temperature and humid conditions. Generally apply 2‑3 coats. Total dry film thickness ≥1.5 mm (subject to design requirements). Theoretical consumption: approx. 2.5‑3.0 kg/㎡.
  4. Curing and Subsequent Procedures After completion of construction, cure naturally for 24‑48 h at normal temperature. Extend curing time under low‑temperature and high‑humidity conditions. No treading, rain exposure or water immersion before full curing. After acceptance of waterproof layer, protective layer (cement mortar, fine aggregate concrete, etc.) must be applied. This product is not suitable for long‑term direct exposure. Water‑storage test: carry out closed‑water test only after full curing of the waterproof layer.

Performance Indexes

No. Inspection Item Technical Requirement
1 Appearance After stirring, the sample shall be uniform without color difference, gel, agglomerate and obvious asphalt filaments
2 Solid content, % ≥45
3 Heat resistance No flowing, slipping or dripping at 110 ℃
4 Surface drying time, h ≤8
5 Hard drying time, h ≤24
6 Low‑temperature flexibility Standard condition No crack or fracture at 0 ℃
7 Elongation at break Standard condition, % ≥600

 

Get in Touch

Have questions about our products or want to discuss a custom order? Our team is ready to help you.

Company Weifang Shihua Chemical Building Material Co., Ltd.
Location Shouguang City, Shandong Province, China
Contact Person Faye Wang

Request A Quote

Please check your email address.
Your message must be at least 20 characters.